LM Comp. Rotation Resistant Wire Rope GB35X7 (6/1)
Please feel freely to contact with us for new price .
产品详情
35x7compacted wire rope construction is available in both galvanised and ungalvanised finish,including 32X7 and 37X7。Depending upon your requirement for higher breaking load or better wear characteristics, these wire ropes are available in different finishes and lubrications as well as being available with plastic impregnated or in compacted constructions.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Offshore crane rope
Deck crane rope
Pillar crane rope
Whip hoist rope
Main hoist rope
Crane rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.7 | 115 | 11699 | 127 | 12961 |
| 13 | 0.82 | 135 | 13730 | 149 | 15212 |
| 14 | 0.95 | 156 | 15924 | 173 | 17642 |
| 15 | 1.09 | 179 | 18280 | 199 | 20252 |
| 16 | 1.24 | 204 | 20798 | 226 | 23043 |
| 18 | 1.57 | 258 | 26323 | 286 | 29163 |
| 20 | 1.94 | 319 | 32497 | 353 | 36004 |
| 22 | 2.35 | 386 | 39322 | 427 | 43565 |
| 24 | 2.79 | 459 | 46796 | 508 | 51846 |
| 26 | 3.28 | 538 | 54921 | 597 | 60847 |
| 28 | 3.8 | 624 | 63695 | 692 | 70568 |
| 30 | 4.37 | 717 | 73119 | 794 | 81009 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.