LM Rotation Resistant Wire Rope GB 32X7 (6/1)
Please feel freely to contact with us for new price .
Product Details
32X7 is available in both galvanised and ungalvanised finish with either ordinary or langs lay. The construction family includes: 34X7, 35X7 and 37X7.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Offshore crane rope
Deck crane rope
Pillar crane rope
Whip hoist rope
Main hoist rope
Crane rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads
|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
mm | kg/m | KN | Kg |
| 8 | 0.29 | 45.2 | 4606 |
| 9 | 0.37 | 57.2 | 5829 |
| 10 | 0.45 | 70.6 | 7197 |
| 11 | 0.55 | 85.4 | 8708 |
| 12 | 0.65 | 102 | 10363 |
| 13 | 0.77 | 119 | 12163 |
| 14 | 0.89 | 138 | 14106 |
| 15 | 1.02 | 159 | 16193 |
| 16 | 1.16 | 181 | 18424 |
| 18 | 1.47 | 229 | 23318 |
| 19 | 1.64 | 255 | 25981 |
| 20 | 1.82 | 282 | 28788 |
| 22 | 2.2 | 342 | 34834 |
| 24 | 2.62 | 406 | 41455 |
General Engineering Ropes
绿盟(LM)专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
简体中文
English