Structural Profiles - Solid Round Rod (Isophthalic)

Structural Profiles - Solid Round Rod (Isophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Nantong Greenlogy TEC Electronic Technology Co., Ltd.

  FRP pultruded profiles are made from glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the surfacing reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold and pulled by a haul-off machine to produce a new type of composite material with good physical properties, widely used in high-strength, long-span applications.  

Solid fiberglass reinforced polymer round rod profile by Greenlogy TEC

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Solid Round Rod

D
D
SRR6060.081/4"0.18
SRR959.50.143/8"0.31
SRR12712.70.261/2"0.57
SRR25425.411"2.2
SRR32831.81.515/4"3.33
SRR380382.153/2"4.74
SRR424.20.033/16"0.07
SRR808.00.15/16"0.22
SRR16160.415/8"0.9
SRR19190.553/4"1.21
SRR20200.6213/16"1.37
SRR22220.727/8"1.59

Markets

Greenlogy TEC FRP profiles used in construction market applications

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Electrically and thermally non-conductive

  • High specific strength

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, good performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded fiberglass structural profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with low thermal conductivity and electrical insulation. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical Properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face

*Only applicable to ISOFR and VEFR


Application Scenarios

Isophthalic solid round rods are commonly used for support, connection and load-bearing components that require both strength and corrosion resistance, such as platform handrail posts, grating support rods, equipment tie rods and various structural reinforcements. In high-humidity, acid-base or salt-spray environments, the isophthalic resin system can provide more stable long-term performance, making it suitable for working conditions in chemical, water treatment, marine and power industries. For specific application recommendations, please contact us to confirm based on your working conditions.

Selection Guide

When selecting, focus mainly on the required diameter, load form (tension/compression/bending), support span and the corrosion level of the service environment, and use these to determine the required cross-sectional size and resin system. Isophthalic solid round rods are more suitable for occasions with stronger corrosiveness or higher durability requirements; for general indoor structures, cost can be evaluated comprehensively. You are welcome to contact us with your working condition parameters so we can help match the appropriate specifications.

Product Advantages

This product uses glass fiber as reinforcement and resin as matrix, and is formed by impregnation, heating curing and pultrusion. It features light weight, high strength, corrosion resistance, electrical insulation and non-magnetic properties, and is easy to cut and machine. The solid round rod has a dense cross-section, stable compressive and flexural performance, and is convenient for drilling, turning and combined installation with other structural parts. Compared with traditional metal materials, it can reduce maintenance requirements in corrosive environments.

Inquiry Guidance

If you would like to know the detailed specifications, size range, resin system options and supply information of this series of solid round rods, please contact us. We will provide selection recommendations and quotation proposals according to your working conditions. You may also provide the required diameter, length, quantity and service environment so that we can reply faster.

Service Environment

  • This solid round rod is produced with isophthalic resin, offering enhanced water resistance and broad resistance to corrosive media, and is suitable for indoor and outdoor installation.
  • Typical service environments for this FRP structural profile include humid and chemical exposure areas, such as industrial plants, wastewater treatment facilities, and marine or coastal areas where steel would corrode.
  • The pultruded glass fiber reinforced structure allows this round rod to be used over a wide temperature range without losing structural integrity; please contact us for detailed temperature performance data.
  • Because the material is non-conductive and corrosion resistant, it is often used in applications near acids, alkalis, salts and other aggressive media; specific chemical compatibility should be confirmed with our technical team.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.