  Pultruded FRP structural profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, the material is heated, formed and cured in a metal mold and pultruded by a pulling machine. It has good physical properties and is widely used in high-strength and long-span applications.  

Greenlogy TEC VEFR-25 FRP rectangular flat tube profile

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Rectangular Tube

A*B*T1*T2


A*B*T1*T2


FT4444*25*3.2*3.20.8

7/4" x 1" x 1/8" x 1/8"

1.76
FT50A51*25*3*30.79

2" x 1" x 1/8" x 1/8"

1.74
FT50B51*25*6.4*6.41.54

2" x 1" x 1/4" x 1/4"

3.4
FT7676*35*3*61.55

3" x 11/8" x 1/8" x 1/4"

3.42
FT8080*60*5*52.5

25/8" x 19/8" x 3/16" x 3/16"

5.51
FT91A91*38*4*41.78

7/2" x 3/2" x 3/16" x 3/16"

3.92
FT112A112*91*6.4*6.44.46

9/2" x 7/2" x 1/4" x 1/4"

9.83
FT120120*45*3*32

19/4" x 7/4" x 1/8" x 1/8"

4.41
FT175175*50*9*97

55/8" x 2" x 3/8" x 3/8"

15.4

Markets 

FRP flat tube profile applications and market uses

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Non-conductive, thermally insulating

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali, and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type with excellent performance, moderate acid/alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

Greenlogy TEC general-purpose acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability, and lightweight properties, while also offering thermal insulation and electrical non-conductivity. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas that traditionally used steel, aluminum, or wood components. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.  

Greenlogy TEC profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, Longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, Transverse

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, Longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, Transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, Longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, Transverse

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, Longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, Transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, Longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, Transverse

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, Longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, Transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic Modulus

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punching Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact Strength, Longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact Strength, Transverse

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding Round Bars and Square Bars

Physical Properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Maximum percentage

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, longitudinal

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical Properties

ASTM

Unit

Value

Arc resistance, longitudinal

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW=longitudinal, CW=crosswise, PF=perpendicular to laminate surface

*Only applicable to ISOFR and VEFR


Application Scenarios

Structural profile – rectangular tube (vinyl) is widely used in chemical, marine, power and other fields with high corrosion resistance requirements, commonly found in platform handrails, support structures, walkway grating frames, etc. The rectangular tube cross-section facilitates connection and installation, making it suitable for applications requiring light weight, high strength, insulation and non-magnetic properties.

Selection Guide

When selecting, please choose based on actual load, span and operating environment, combined with the cross-sectional dimensions and wall thickness of the rectangular tube. We offer a variety of specifications to meet different structural requirements. For precise selection advice, please contact us for detailed specifications and technical support.

Product Advantages

Made with vinyl resin, it offers excellent corrosion resistance and weather resistance; glass fiber reinforcement gives it high strength and light weight. The pultrusion process ensures stable dimensions and a smooth surface, along with advantages such as insulation, non-magnetic properties and low maintenance.

Inquiry Guide

For detailed specifications, pricing and supply information on structural profile – rectangular tube (vinyl), please contact us for detailed specifications and a quotation. Our technical team will provide professional selection advice and customized solutions.

Operating Environment

  • This FRP rectangular tube is suitable for both indoor factory installation and outdoor structural frameworks, where pultruded FRP profiles resist moisture and do not corrode like steel.
  • The vinyl resin system makes this rectangular tube suitable for continuous use in humid or chemically corrosive atmospheres, including areas with acids, alkalis or salts.
  • Typical operating conditions include walkway supports, handrail infill and platform frames, where the rectangular tube carries loads across spans while exposed to weather or washdown environments.
  • Because the glass fiber reinforcement is fully impregnated and cured during the pultrusion process, this rectangular tube maintains its shape and strength through temperature fluctuations from high-temperature process areas to cold outdoor sites; please contact us with your actual operating temperature and media for project-specific recommendations.