FRP Molded Grating 19*19H25

FRP Molded Grating 19*19H25

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---


Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type

Software - Sample 3 for three columns

Shop sand type

19 19 H25

19*19*25(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):6.5/5.0

Bearing bar center:19

Open Aera:40%

Approx Weight:16.8kgs/m²

19 19 H25

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP Molded Grating 19*19H25 offers excellent corrosion resistance, slip resistance and load-bearing performance, making it suitable for operating platforms, walkways, drainage trench covers and stair treads in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its lightweight and high-strength characteristics also make it easy to install and remove, ideal for locations requiring frequent maintenance.

Selection Guide

When selecting, consider load-bearing requirements, span, corrosivity of the service environment and flame-retardant grade. Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) correspond to different corrosion resistance and flame-retardant performance, so the appropriate resin system can be chosen according to specific working conditions. Please contact us for detailed specifications and selection advice.

Product Advantages

FRP molded grating is formed in a single molding process, with good structural integrity, high strength and light weight, only about 1/4 that of steel grating. Its surface has anti-slip protrusions, and anti-slip materials such as quartz sand can be added as required. The product resists corrosion from various chemical media, has a long service life and low maintenance cost, and offers good insulation and non-magnetic properties.

Inquiry Guide

For detailed specifications, prices and supply information of FRP Molded Grating 19*19H25, please contact us for professional consultation and quotation. We can provide customized solutions according to your specific needs.

Operating Environment

  • Molded FRP grating with a 19×19 mm mesh and 25 mm depth is used in industrial plants, water treatment facilities and chemical processing areas where the working environment may be humid, wet or subject to occasional splashes.
  • The unsaturated polyester resin matrix resists many corrosive media found in process industries, making the grating suitable for both indoor installations and outdoor platforms exposed to weather.
  • With an oxygen index up to about 80 for phenolic-type resin, the grating is intended for locations where fire safety is a primary concern, such as areas with flammable materials or high-temperature processes.
  • For detailed chemical resistance data, temperature limits and UV performance in your specific operating conditions, please contact us with your application details.

Custom Cutting