  Pultruded FRP grating is made with pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, assembled through a certain assembly process into grating with gaps left in the panel surface.  

Name

Contact Information

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass Fiber

65%

E

Filler

8%

ATH,PR

Other

2%

---

Raw Material Introduction 
Resin Type

Code

Resin Type

Flame Retardancy

Recommended Applications

MP-5

Phenolic Type

Oxygen index can reach about 80

Low toxicity, high flame retardancy, suitable for applications with high fire-safety requirements

VEFR-25

Vinyl Ester Type

Oxygen index 28 and above

Harsh environments with strong acid, alkali and other corrosive media

VEFR-10

Vinyl Ester Type

Oxygen index 35 and above

Strong acids, strong alkalis and other demanding applications where higher flame retardancy is required

IFR-25

Isophthalic Type

Oxygen index 28 and above

VEFR economical type, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Benzene-based, food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame retardancy requirement

Coarse glass fiber type selection   

Code

Coarse grit type

Recommended Applications

E

Alkali-free glass grit

For applications requiring high strength and high corrosion resistance

Filler type selection 

Code

Filler type

Recommended Applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For highly corrosion-resistant applications

Software - three-column example 1

Sand surface
Software - three-column example 2

Smooth surface
Software - three-column example 3

Anti-slip grooved surface

T3310

Standard panel size:
Width 1220mm, 915mm; length 3050mm, 6100mm
Bearing bar: 25mm
Open area: 33%

Approx. weight (incl. three cores): 11.2kg/m²
Diagram showing line load distribution on a pultruded grating span

Line load (unit: mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

300450750150030005950

Load

4500.580.861.452.875.74---10309
6001.271.933.236.45------7731
9004.015.9910.1---------5024
12008.99---------------3620
Diagram showing uniformly distributed load across a pultruded grating panel

Uniformly distributed load (unit: mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

1000190039007000950019500

Load

4500.561.072.134.045.23---45076
6001.633.236.5412.1------25363
9007.5215------------10971
1200------------------5938

Features:

  • Flame retardant

  • Highly flame retardant

  • Low smoke, non-toxic gas release

  • High strength-to-weight ratio

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Non-conductive and thermally insulating

  • Easy to fabricate

  • Impact resistance 

  • UV resistance

  • Maintenance-free

Installation and accessories 

Installation and accessories

Applications

Pultruded Grating T-3310 is suitable for platforms, walkways, trench covers, stair treads and equipment operating surfaces that require a combination of load-bearing capacity, corrosion resistance, and ventilation and drainage. It is commonly used in chemical, water treatment, electroplating, marine engineering and power applications involving damp, acid-base or salt-spray environments. If your operating conditions involve high temperatures, severe corrosion or special loads, please contact us to confirm a suitable solution based on the specific medium, span and installation method.

Selection guide

When selecting, we recommend first clarifying the resin system (such as OFR, IFR, VEFR or phenolic types, corresponding to different flame-retardant and corrosion-resistance orientations), the load-bearing direction and the support span, then confirming the grating thickness, mesh spacing and connection method to match the actual load and installation conditions. Because different resin and fiber ratios affect strength, flame retardancy and corrosion resistance, please contact us with your operating parameters and we will assist with selection and specification confirmation. For detailed specifications and quotations, please contact us.

Product advantages

Pultruded Grating T-3310 uses pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, combined with solid tubes or rods as connecting rods, assembled according to a certain process with gaps left in the panel surface, so it combines relatively high longitudinal load-bearing capacity with light weight, corrosion resistance and ease of cutting and installation. This structure facilitates ventilation, drainage and light transmission, and is non-conductive and non-magnetic, making it suitable as a replacement for some metal gratings in corrosive environments. Specific performance varies with resin and fiber configuration; please contact us to confirm the applicable configuration.

Inquiry prompt

For further information on the detailed specifications, resin selection recommendations and commercial terms of Pultruded Grating T-3310, please contact us and provide your operating environment, load requirements and dimensional needs; we will provide a targeted solution and quotation accordingly. Please contact us for detailed specifications and quotations.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.