FRP Grating and Wire Rope Guides

Every technical guide we publish on FRP grating and wire rope - selection, sizing, data and applications - collected in one place.

These guides answer the questions our engineers hear most often: which grating type suits an application, how to read load tables, what the specifications mean, and how wire rope construction and finish affect performance in service.

Every guide is written by our technical team from the products we build and the questions customers ask, and each one links to the matching products in our shop.

FRP Grating Guides

Molded vs Pultruded FRP Grating

How the two manufacturing routes differ in construction, load capacity, corrosion performance and cost - and which to choose.

Load Capacity and Deflection

How to read FRP grating load tables: linear and uniform load data, deflection values, and how to pick a mesh for your span.

Specifications and Sizes

Molded mesh sizes, panel dimensions, open area, weight, resin systems and surface options - the full product data in one place.

Anti-Slip Grating and Stair Treads

Grooved, sanded and polished anti-slip surfaces compared, plus molded FRP stair treads for safe footing in wet and oily areas.

FRP vs Steel Grating: How to Choose

Corrosion, weight, strength, fire performance and cost - how to choose between FRP and steel grating for your application.

Wire Rope Guides

Wire Rope Construction Guide

What 6x19 and 6x36 mean, how 1x19, 7x19 and rotation-resistant ropes behave, and which construction fits your application.

Galvanized Wire Rope

How zinc coating protects steel, hot-dip vs electro-galvanized, and when to choose galvanized over bright or stainless steel.

Stainless Steel Wire Rope

304 vs 316 marine grade, available constructions and breaking strengths, and where stainless beats galvanized for corrosion.

Wire Rope Core Types: FC vs IWRC

How fiber core and steel core differ in strength, flexibility and crush resistance, with same-diameter data for 6x36, 6x19 and 6x37.

Breaking Strength and Safe Working Load

MBL vs safe working load, wire grades, and breaking strengths for 1x19, 6x36 and rotation-resistant ropes.

Application Guides

Metals and Mining

Grating, platforms, profiles and technical services for mines, smelters and metals plants.

Chemical Industry

Resin selection, structural design and application for chemical-resistant FRP grating and platforms.

Docks and Decking

Corrosion-proof FRP grating and pultruded profiles for docks, decks, marinas and industrial walkways.

Water and Wastewater

Corrosion-resistant grating, access solutions and technical services for treatment plants and water facilities.

Oil and Gas

FRP platforms, stair treads and profiles for refineries, terminals and offshore duty.

Utilities and Power

FRP products and technical services for substations, power plants and utility walkways.

Looking for your industry? Browse all applications and industries.

Ordering and Payment

How to Order and Payment Terms

How an order runs from inquiry to shipment: quotation and lead time, trade terms, third-party inspection, LCL and FCL shipping, free samples, payment terms and the company bank account.

Custom Cutting to Size

Panels cut to size, edges sealed with resin and holes pre-drilled to your drawing before shipping. Cut to shape and wire rope cut to length too.

Frequently Asked Questions

What do the guides cover?

Every technical guide we publish on FRP grating and steel wire rope - selection, sizing, load and breaking-strength data, corrosion performance and applications - collected in one place.

Which guide should I read first?

Start with the selection guides: molded vs pultruded for FRP grating, and wire rope construction for steel wire rope. They set out the vocabulary the other guides build on.

Do the guides cover both FRP grating and steel wire rope?

Yes. The library follows our product lines: FRP grating for walkways, platforms and stairs, and steel wire rope for lifting, rigging and anchoring, with data tables and application notes for each.

Where do the numbers in the guides come from?

The load tables, breaking strengths and dimensions follow the standards our products are made to, such as GB/T 20118 for wire rope, and match our standard product data. For a specific project, send us the duty and we will confirm the figures for your case.

How do I get a quotation or ask a technical question?

Every guide links to the matching product pages, and each product page has a quotation form. Send your inquiry there and our engineers reply with the specification, price and lead time.

Need help choosing the right product for your application? Send your duty and environment to admin@greenlogy.cn, or browse the FRP grating range and the wire rope range.

Wire Rope Sizes: Breaking Strength by Diameter

Each inch size has its own page, built from the same product tables as the chart above: the breaking load of every construction we stock at that size, the working load at 5:1, 6:1 and 8:1, and what to write on the enquiry.

1/8" wire rope: breaking strength and working load — 3.2 mm, MBL 5–9.26 kN, 5:1 working load 1–1.9 kN.

3/16" wire rope: breaking strength and working load — 4.8 mm, MBL 13.9–25.7 kN, 5:1 working load 2.8–5.1 kN.

1/4" wire rope: breaking strength and working load — 6.4 mm, MBL 20–37 kN, 5:1 working load 4–7.4 kN.

5/16" wire rope: breaking strength and working load — 7.9 mm, MBL 35.6–65.9 kN, 5:1 working load 7.1–13.2 kN.

3/8" wire rope: breaking strength and working load — 9.5 mm, MBL 55.6–103 kN, 5:1 working load 11.1–20.6 kN.

1/2" wire rope: breaking strength and working load — 12.7 mm, MBL 80–148 kN, 5:1 working load 16–29.6 kN.

5/8" wire rope: breaking strength and working load — 15.9 mm, MBL 161–263 kN, 5:1 working load 32.2–52.6 kN.

1" wire rope: breaking strength and working load — 25.4 mm, MBL 426–696 kN, 5:1 working load 85.2–139.2 kN.

Rotation-Resistant Wire Rope

Rotation-Resistant Wire Rope: 18x7 to 37x7

What each construction does, the published breaking load of all eleven products at 16 mm, compaction and coating, and the duty each construction is listed for.