FRP Grating 38*38H38
Request a Quote
Please feel freely to contact with us for new price .
Nantong Greenlogy Electronic Technology Co., Ltd. (Greenlogy TEC)
Fiberglass reinforced plastic (FRP) grating is a panel with a certain open area, custom molded using unsaturated polyester resin (including isophthalic, phenylene, phenolphthalein, and bisphenol types) as the skeleton.
Code | Resin type | Flame retardant performance |
Recommended applications |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardancy, for applications where fire safety is extremely important |
VEFR-25 | Vinyl ester type | Oxygen index 28 or above | In severely corrosive environments such as acids, alkalis, and solvents |
VEFR-10 | Vinyl ester type | Oxygen index 35 or above | Applications requiring high flame retardancy along with excellent acid and alkali resistance |
IFR-25 | Isophthalic type | Oxygen index 28 or above | More economical than VEFR type, with excellent acid resistance and moderate alkali and solvent resistance |
IFGR-30 | Isophthalic food grade | Oxygen index 26 | Mainly used in meat processing and food processing plants |
FR-25 | Orthophthalic type | Oxygen index 28 or above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | More economical than OFR-25, no flame retardancy requirement |
Type of glass fiber roving selected
Code | Roving type | Recommended applications |
E | E-glass roving | Applications requiring higher strength and corrosion resistance |
Type of filler selected
Code | Filler type | Recommended applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing, corrosion-resistant applications |
PR | No filler, pure resin | For highly corrosion-resistant applications |




38*38*38(mm)
Panel size:
1220*4000,1220*3660,1220*2440,
915*3050,1524*3050,
1524*4000
Bidirectional load-bearing.
Rib wall thickness (top, bottom) 7.0/5.0
Load-bearing bar center spacing: 30
Open area: 68%
Approximate weight per square meter: 19.5 kgs/㎡
Linear load (unit: mm)
| Deflection | kg/m | Ultimate | |||||
|---|---|---|---|---|---|---|---|
| Span (mm) | 150 | 300 | 450 | 600 | 750 | 1500 | Load |
| 300 | 0.36 | 0.48 | 0.61 | 0.76 | 0.89 | 1.06 | 17116 |
| 600 | 0.66 | 1.25 | 1.85 | 2.46 | 3.07 | 8.48 | 8718 |
| 900 | 1.80 | 3.68 | 5.56 | 7.42 | 9.30 | 13.8 | 5817 |
| 1200 | 4.75 | 9.68 | 14.6 | 19.6 | 21.2 | --- | 3755 |



Operating Environment
- Designed for outdoor and indoor industrial environments: this 38*38H38 molded FRP grating is made from unsaturated polyester resin and withstands weathering, UV exposure and humid conditions without the corrosion problems commonly seen with steel grating in open workshops, walkways and platforms.
- Suitable for highly chemically corrosive environments: the resin systems used in this FRP grating (isophthalic, phenylene, bisphenol and related types) are selected to resist acids, alkalis, salts and other corrosive media present in chemical, wastewater treatment and processing areas.
- For environments where fire performance is a concern, flame-retardant resin grades are available: the phenolic type has a high oxygen index, making the grating suitable for applications requiring low toxicity and high flame retardancy.
- Suitable for environments with temperature and humidity variations commonly found in workshop floors, cooling towers, marine and coastal sites, and washdown areas; please contact us for recommended resin grades and full parameter tables for your specific operating conditions.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文