FRP Molded Grating 83*83 H25

FRP Molded Grating 83*83 H25

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---


Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Feature One

Software - Sample 2 for three columns

Feature Two

Software - Sample 3 for three columns

Feature Three

83 83 H25

83*83*25(mm)

Panel size available:

1007*4007,1007*3007 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:83

Open Aera:84%

Approx Weight:5.8kgs/m²

83 83 H25

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 83*83 H25 is suited to platforms, walkways, trench covers and equipment operating surfaces that require corrosion resistance, high strength-to-weight ratio and slip resistance, and is commonly found in chemical, water treatment, power and marine engineering environments. Its 25 mm thickness and 83*83 mm mesh strike a balance between load capacity and openness, making it suitable for medium-to-light load access and drainage scenarios. For suitability under specific working conditions, please contact us to confirm based on your site conditions.

Selection Guide

Selection can start from several dimensions: load requirements, span, corrosive media, flame retardant requirements and installation method. The resin system affects corrosion resistance and flame retardant performance; grating thickness and mesh size affect load capacity and self-weight; surface treatment affects slip resistance and appearance. If you provide the service environment and load conditions, we can help recommend a suitable resin type and structural solution. For detailed specifications and selection advice, please contact us.

Product Advantages

Molded grating is formed in one piece from resin and fiberglass, offering general advantages such as light weight and high strength, corrosion resistance, non-conductivity and low maintenance, while the mesh structure allows water and air to pass through and reduces dirt accumulation. Compared with traditional metal grating, it is more durable in damp or corrosive environments, and is also relatively easy to install and cut. Actual performance is subject to the selected specification and test reports; please contact us to learn more.

Inquiry Guidance

For detailed specifications, resin options, pricing and delivery information on FRP molded grating 83*83 H25, please contact us. Please provide your application scenario, load requirements, dimensions, quantity and any special needs, and we will provide a targeted solution and quotation as soon as possible.

Operating Environment

  • Molded FRP grating with 83 x 83 mm mesh and 25 mm depth is typically installed both indoors and outdoors, where the unsaturated polyester resin system resists moisture, splash and weathering better than bare steel.
  • In chemical plants, wastewater treatment areas and plating shops the grating is used over floors, trenches and walkways where acids, alkalis and salt solutions are handled, so the resin grade (OFR, IFR, VEFR, phenolic or bisphenol type) can be matched to the corrosive medium on site.
  • The E-glass fiber reinforcement and ATH / PR filler help the panel keep its shape under humid, wet or intermittently washed-down conditions, making it suitable for cooling tower surrounds, pump skids and other constantly damp service areas.
  • For open-air platforms, stairs and access ways exposed to sun and rain, the molded grid is chosen where a non-slip, corrosion-resistant surface is required without painting; the exact resin grade and fixing method should be confirmed with us against the actual temperature range and chemical exposure of your project.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp