FRP Molded Grating 83*83H40

FRP Molded Grating 83*83H40

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Feature One

Software - Sample 2 for three columns

Feature Two

Software - Sample 3 for three columns

Feature Three

83 83 H40

83*83*40(mm)

Panel size available:

1007*4007,1007*3007 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:83

Open Aera:84%

Approx Weight:9.5kgs/m²

83 83 H40

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

The combination of 83*83 mesh size and 40mm thickness in FRP molded grating 83*83H40 makes it suitable for industrial platforms, walkways, trench covers and flooring where load-bearing and slip resistance are required. Its open structure allows liquids and debris to pass through, and it is commonly used in corrosive environments such as chemical, water treatment, electroplating and marine engineering.

Selection Guidance

During selection, the resin system and grating thickness should be determined based on actual load, span, support method and service environment. The mesh and thickness parameters of 83*83H40 can be compared with other specifications in our molded grating series. Please contact us for detailed specifications and selection advice.

Product Advantages

FRP molded grating is molded from unsaturated polyester resin and fiberglass, offering characteristics such as light weight, high strength, corrosion resistance, slip resistance and insulation. The 83*83H40 mesh design balances load-bearing capacity and open area, making it easy to install and maintain.

Inquiry Guidance

If you need to know the resin type, color, surface treatment and packaging method of FRP molded grating 83*83H40, please contact us for detailed specifications and quotation. We can provide customized solutions according to your project requirements.

Operating Environment

  • This molded FRP grating is built for both indoor and outdoor installations, such as walkways, platforms and stair treads in chemical plants, wastewater treatment facilities and offshore environments, where the unsaturated polyester resin matrix resists moisture and humidity.
  • The isophthalic, vinyl ester and bisphenol-A type resins offer resistance to corrosive media including acids, alkalis and salts, making the grating suitable for areas with chemical splashes or fumes.
  • With a flame-retardant formulation available (OFR-25, IFR-25, VEFR-25 and phenolic type), this grating is intended for applications where fire safety is a concern.
  • For specific temperature ranges, chemical concentration limits and service conditions, please contact us for the full parameter list and application guidance.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp