LM (Coating) Comp. Rotation Resistant Wire Rope GB32X7 (6/1)
Request a Quote
Please feel freely to contact with us for new price .
Product Details
32x7 compacted wire rope is available in galvanized and non-galvanized versions, and 34x7, 35x7 and 37x7 specifications are also available. According to your requirements for higher breaking load and better wear characteristics, we can apply surface treatment, lubrication, plastic coating and compaction.
Surface treatment: bright or galvanized
Standard: National Standard GB/T 20118-2006

Engineering Applications
Offshore crane wire rope
Deck crane wire rope
Column crane wire rope
Lifting sling
Main hoist wire rope
Sling
Breaking load
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load | |
|---|---|---|---|---|---|
Diameter | Weight |
(1960Mpa) |
(1960Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.32 | 50 | 5100 | 55 | 5610 |
| 11 | 0.6 | 95 | 9690 | 105 | 10710 |
| 12 | 0.71 | 111 | 11322 | 123 | 12546 |
| 13 | 0.84 | 132 | 13464 | 146 | 14892 |
| 14 | 0.97 | 153 | 15606 | 169 | 17238 |
| 15 | 1.1 | 174 | 17748 | 193 | 19686 |
| 16 | 1.25 | 198 | 20196 | 219 | 22338 |
| 18 | 1.61 | 255 | 26010 | 282 | 28764 |
| 19 | 1.8 | 284 | 28968 | 315 | 32130 |
| 20 | 1.97 | 310 | 31620 | 344 | 35088 |
| 22 | 2.36 | 372 | 37944 | 412 | 42024 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications, with fiber core and steel core options. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes are designed to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and comply with ISO9001.
Selection Guide
When selecting, please consider the rated load of the lifting equipment, the diameter ratio of sheave to drum (D/d), the operating environment (such as offshore, humid or corrosive conditions) and the required rope diameter to determine the surface treatment (bright or galvanized) and whether additional processes such as plastic coating or compaction are needed. You can provide us with the specific working parameters, and our technical team will assist in matching specifications such as 32x7, 34x7, 35x7 and 37x7.
Product Advantages
This series of wire rope features a compacted structure, offering higher breaking load and good anti-rotation and wear resistance, suitable for offshore cranes, deck lifting, column cranes and main hoisting applications. The choice of galvanized and non-galvanized versions adapts to different anti-corrosion requirements, and processes such as surface treatment, lubrication, plastic coating and compaction can be customized on request.
Inquiry Guidance
Welcome to contact us for detailed specifications, breaking load data sheets, surface treatment options and quotation proposals. Please provide the required diameter, length, surface treatment method and operating conditions, and we will provide targeted recommendations and commercial terms accordingly.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

简体中文