6x36 wire rope is available with either FC (fiber core) or IWRC (independent wire rope core), and is a general-purpose flexible engineering wire rope. This wire rope offers superior breaking load capacity and good fatigue resistance, with a long service life and wide application.

Surface finish: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy TEC GB (Coated) Compacted Wire Rope 6x36 (14/7+7/7/1) FC

Engineering Applications

  • General engineering applications

  • Grab crane ropes

  • Wire rope slings

  • Crane ropes

  • Slings

  • Winch ropes

  • Lifeboat ropes

  • Mooring ropes

  • Search ropes

  • Luffing ropes

  • Traction ropes

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

 (1960Mpa)

 (1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

80.2437.4381341.44222
90.347.3482552.45343
100.3758.4595764.76597
110.4470.7720878.37982
120.5384.1857993.19500
140.721141167712712930
160.941501525216616889
181.191891930321021375
201.472342383125926389
221.782832883531331931
242.113363431737338000
262.483954027443744598
282.884584670950751723
303.35265362058259376
323.765986100866267556
344.246756887274876265
364.767577721383885501
385.38438603093495265
405.87935953251035105557
426.4710301050951141116377
447.1111311153431252127724
467.7712361260671369139600
488.4613461372681490152003
509.1814601489451617164934
529.9215791610991749178392
5611.518321868372020206893
6013.221032144812328237504

General engineering wire rope

   Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.

Most wire ropes operate under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes are designed to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with assembly components such as thimbles, swaged ends and wedge sockets, among many others. We also offer customization services: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and conform to ISO9001.


Selection Guidance

Please determine the wire rope diameter, core type (FC fiber core or IWRC steel core) and strength grade of 1770MPa or 1960MPa based on the actual working conditions, including working load, sheave or drum diameter, corrosive environment and required safety factor. If you have high requirements for bending fatigue life or crushing resistance, we recommend providing detailed operating conditions so we can assist with selection. Contact us for structural and specification recommendations for your specific application.

Product Advantages

The 6x36 construction combines flexibility with load-bearing capacity. The FC fiber core provides good bendability, making it suitable for general engineering applications involving frequent bending. The surface is available in bright or galvanized finish to suit different environmental conditions. The product offers long service life and good fatigue resistance, and can be used in applications such as slings, cranes, winches and mooring. Please evaluate specific performance based on actual operating conditions.

Inquiry Guidance

Contact us for detailed specifications, diameter and length options, surface treatment methods and quotation information. For bulk purchases or custom constructions, please inform us of your application scenario and technical requirements, and we will provide further support accordingly.

Cut to Length

Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

WhatsApp