LM (Coating) Fiber Core Wire Rope GB6X36 FC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is available with FC (fibre core) or IWRC (independent wire rope core), and is a general-purpose flexible engineering wire rope. This wire rope offers superior breaking load capacity and good fatigue resistance, with a long service life and wide application.
Surface treatment: bright, galvanized or 316 marine-grade stainless steel
Standard: GB/T 20118-2006

Engineering applications
General engineering applications
Grab crane ropes
Wire rope slings
Crane ropes
Slings
Winch ropes
Lifeboat ropes
Mooring ropes
Search ropes
Luffing ropes
- Traction ropes
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.24 | 37.4 | 3813 | 41.4 | 4222 |
| 9 | 0.3 | 47.3 | 4825 | 52.4 | 5343 |
| 10 | 0.37 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.44 | 70.7 | 7209 | 78.3 | 7982 |
| 12 | 0.53 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.62 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.72 | 115 | 11677 | 127 | 12930 |
| 15 | 0.83 | 131 | 13405 | 146 | 14844 |
| 16 | 0.94 | 150 | 15252 | 166 | 16889 |
| 18 | 1.19 | 189 | 19303 | 210 | 21375 |
| 19 | 1.33 | 211 | 21507 | 234 | 23816 |
| 20 | 1.47 | 234 | 23831 | 259 | 26389 |
| 22 | 1.78 | 283 | 28835 | 313 | 31931 |
| 24 | 2.11 | 336 | 34317 | 373 | 38000 |
| 26 | 2.48 | 395 | 40274 | 437 | 44598 |
| 28 | 2.88 | 458 | 46709 | 507 | 51723 |
| 30 | 3.3 | 526 | 53620 | 582 | 59376 |
| 32 | 3.76 | 598 | 61008 | 662 | 67557 |
| 34 | 4.24 | 675 | 68872 | 748 | 76265 |
| 36 | 4.76 | 757 | 77213 | 838 | 85501 |
| 38 | 5.3 | 843 | 86030 | 934 | 95265 |
| 40 | 5.87 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.47 | 1030 | 105095 | 1141 | 116377 |
| 44 | 7.11 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.77 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.46 | 1346 | 137268 | 1490 | 152003 |
General engineering wire rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized steel wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and abrasion. All our wire ropes are designed to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and conform to ISO9001.
Selection Guide
This 6x36 wire rope is available with either FC (fiber core) or IWRC (independent wire rope core), and can be supplied in bright, galvanized or 316 marine-grade stainless steel finish. When selecting, determine the core type and finish based on the flexibility requirements, fatigue resistance needs and environmental corrosion conditions of your application. For breaking load and weight data for specific diameters, please contact us for detailed specifications and a quotation. The product conforms to GB/T 20118-2006 and is suitable for general engineering, grab cranes, slings, winches and mooring applications.
Product Advantages
The 6x36 construction gives the wire rope good flexibility and fatigue resistance, and the FC or IWRC core options balance breaking load capacity with service life. The finish options (bright, galvanized, 316 marine-grade stainless steel) suit different corrosive environments, meeting diverse needs from general lifting to marine engineering. This product complies with GB/T 20118-2006 and is a general-purpose choice for cranes, slings, winches and mooring applications.
Inquiry Guide
For detailed technical parameters, packaging methods and commercial terms corresponding to specific diameters, core types and finishes, please contact us. Please provide the required diameter, core type (FC or IWRC), finish requirements and estimated quantity, and we will recommend suitable specifications based on your working conditions and provide a quotation.
Operating Environment
- GB6X36 FC wire rope with fibre core is suited to general outdoor and indoor engineering use where the rope is exposed to weather, humidity and temperature variation, including construction sites, ports and plant yards.
- The fibre core construction makes the rope a practical choice for running and lifting duties on cranes, grab cranes and winches, where the rope passes over sheaves and drums and must tolerate repeated bending in dusty or damp surroundings.
- For mooring, lifeboat and other marine or offshore duties, the galvanized or 316 marine-grade stainless steel surface treatment of this rope is available to resist corrosive media such as salt-laden air and water splash.
- When a job involves continuous outdoor exposure, abrasive contact or other aggressive conditions, the appropriate surface treatment and rope diameter should be selected according to the working environment; contact us for the full parameter list and selection guidance.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.