LM (Coating) Fiber Core Wire Rope GB6X37 FC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
The 6x37 specification is generally used for cross-laying in engineering. In addition to fiber core, IWRC (independent wire rope core) is also available. 6x36 is more popular in the UK, while on the European continent, the 6x37 specification is generally used.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006

Engineering Applications
General Engineering Wire Rope
Crane Wire Rope
Slings
Breaking Load
|
|
Minimum Breaking Load |
Minimum Breaking Load |
Minimum Breaking Load | Minimum Breaking Load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.5 | 75.2 | 7669 | 83.3 | 8492 |
| 13 | 0.59 | 88.2 | 9000 | 97.7 | 9967 |
| 14 | 0.68 | 102 | 10438 | 113 | 11559 |
| 16 | 0.89 | 134 | 13634 | 148 | 15098 |
| 18 | 1.12 | 169 | 17256 | 187 | 19108 |
| 20 | 1.38 | 209 | 21303 | 231 | 23590 |
| 22 | 1.68 | 253 | 25777 | 280 | 28544 |
| 24 | 1.99 | 301 | 30677 | 333 | 33970 |
| 26 | 2.34 | 353 | 36003 | 391 | 39868 |
| 28 | 2.71 | 409 | 41755 | 453 | 46237 |
| 30 | 3.11 | 470 | 47933 | 520 | 53078 |
| 32 | 3.54 | 535 | 54537 | 592 | 60391 |
| 34 | 4 | 604 | 61567 | 668 | 68176 |
| 36 | 4.48 | 677 | 69024 | 749 | 76433 |
| 38 | 5 | 754 | 76906 | 835 | 85161 |
| 40 | 5.54 | 835 | 85214 | 925 | 94362 |
| 42 | 6.1 | 921 | 93949 | 1020 | 104034 |
| 44 | 6.7 | 1011 | 103110 | 1119 | 114178 |
| 46 | 7.32 | 1105 | 112696 | 1224 | 124794 |
| 48 | 7.97 | 1203 | 122709 | 1332 | 135881 |
General Engineering Wire Rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1x19, 7x7, 6x19, 7x19, 6x36, 8x19, 8x36, 19x7 and 35x7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also provide premium special wire ropes.
Most wire ropes work under demanding conditions and must possess resistance to crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life, thereby improving end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets as well as many other assembly components. We also offer customization services, and our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
Selection Guide
When selecting, please consider the load requirements of the working conditions, sheave diameter, operating frequency and environmental corrosion conditions to confirm the required diameter, surface treatment (bright or galvanized) and core type. LM (coated) fiber core wire rope is suitable for general engineering, lifting and sling applications. If higher load capacity is required, IWRC construction can be selected. For specific specifications, please contact us for detailed parameters and selection advice.
Product Advantages
LM coated fiber core wire rope adopts a 6x37 construction with good flexibility, making it easy for cross-laying and reeving. The fiber core helps improve the rope's cushioning and bending performance. The surface can be supplied bright or galvanized to suit different anti-rust requirements. The product is manufactured according to the GB/T 20118-2006 standard and is suitable for general engineering, crane and sling applications.
Inquiry Guide
For detailed specifications, breaking load data, surface treatment options and supply solutions for LM (coated) fiber core wire rope, please contact us for a detailed quotation and technical information. Please provide the required diameter, core type, surface treatment and working conditions, and we will recommend suitable products and commercial terms accordingly.
Operating Environment
- GB6X37 FC fiber core wire rope is used in general engineering, crane and sling applications, which may involve both indoor and outdoor working conditions.
- The fiber core provides flexibility for cross-laying in engineering, but it should be kept away from excessive moisture and aggressive chemicals; for such environments, galvanized or IWRC alternatives may be considered.
- Typical temperature and humidity ranges are those of the surrounding industrial or construction site; no specific values are stated for this product, so contact us for application-specific guidance.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.