LM (Coating) Filler Wire Rope GB6X19(12/6+6F/1) IWRC
Please feel freely to contact with us for new price .
Product Details
6X19 (Coating)filler wire rope (often referred to as 6X25) is available with both FC (fibre core) and IWRC (independent wire rope core). 6X19 filler wire rope can work from 1 tonne load up to 5 tonnes. It is used in the North Sea Oil industry .
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006
.jpg?access_token=7bc144a2-e776-484c-912d-723f5a583b18)
Applications
Drilling ropes
Elevator rope
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Trawl wraps / Pelagic sweeps
Trawl wraps / Pelagic sweeps
Excavator rope / Scraper rope
Fishing rope
Fishing rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.74 | 1220 | 124431 | 1351 | 137788 |
| 46 | 8.46 | 1333 | 136000 | 1477 | 150598 |
| 48 | 9.22 | 1452 | 148083 | 1608 | 163979 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
简体中文
English