LM Marine Grade stainless steel Wire Rope GB7x7 (6/1)
Please feel freely to contact with us for new price .
产品详情
7x7不锈钢钢丝绳比1x19更灵活,比7x19更坚固。在较小直径内,7x7具有优异的断裂载荷和灵活性,在整个海洋工业以及一般工程应用中广泛使用。
Surface treatment:Ungalv  or  Galvanized
Standard:GB/T 20118-2006

Applications
Control cables
Guardrail
Standing rigging
Running rigging
Steering cable
Marine/Saltwater environment
Sewage treatment works
Wire rope slings
Davit ropes
Breaking Loads
Diameter 
  | Weight 
  | 
 Min Breaking Loads(1570Mpa) 
  | 
 Min Breaking Loads(1570Mpa) 
  | 
mm  | kg/m  | KN  | 
 Kg  | 
| 1 | 0.004 | 0.59 | 60 | 
| 2 | 0.016 | 2.37 | 241 | 
| 2.5 | 0.023 | 3.71 | 378 | 
| 3 | 0.034 | 5.34 | 544 | 
| 4 | 0.06 | 9.49 | 967 | 
| 5 | 0.1 | 14.8 | 1509 | 
| 6 | 0.14 | 21.4 | 2182 | 
| 7 | 0.19 | 29.1 | 2967 | 
| 8 | 0.24 | 38 | 3874 | 
| 10 | 0.38 | 59.3 | 6046 | 
| 12 | 0.55 | 85.4 | 8708 | 
| 14 | 0.74 | 117 | 11930 | 
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.