LM Sealed Wire Rope GB6X19(9/9/1) IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x19 locked coil wire rope is available with FC (fiber core) and IWRC (independent wire rope core), offering excellent breaking load characteristics and a wide range of applications. For applications requiring higher abrasion resistance, 6x19 locked coil wire rope is more suitable than other 6x19 wire ropes.
Surface finish: bright or galvanized
Standard: GB/T 20118-2006
.jpg?access_token=a97cb562-0422-4b61-a0dc-73fdaa5e1005)
Engineering applications
Drilling line
Elevator hoisting rope
Wire rope slings
Luffing wire rope
Hoisting rope
Crane wire rope
Sand line, core line and swabbing line
Trawl fishing / ocean sweeping
Grounding rope / ground tow rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing rope
Tow rope
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.4 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.48 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.58 | 90.7 | 9255 | 101 | 10248 |
| 13 | 0.68 | 107 | 10862 | 118 | 12028 |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 15 | 0.9 | 142 | 14461 | 157 | 16013 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
General Engineering Wire Rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with assembly components such as thimbles, swaged terminals, wedge sockets and many others. We also offer customization; our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and conform to ISO9001.
Selection Guide
Selection should take into account factors such as load requirements, operating environment, wear resistance and flexibility. The 6x19 fully locked coil wire rope is available with FC (fiber core) and IWRC (independent wire rope core), and with bright or galvanized surface treatment to suit different working conditions. For specific selection advice, please contact us; our technical team will provide professional guidance based on your application.
Product Advantages
The 6x19 fully locked coil wire rope is produced to the national standard GB/T 20118-2006, offering excellent breaking load characteristics. It is more wear-resistant than other 6x19 wire ropes, making it suitable for applications with high wear resistance requirements. Its structural design balances strength and flexibility, and it is widely used in drilling lines, elevator hoisting ropes, crane ropes and many other engineering fields.
Inquiry Guide
If you have any questions about the specifications, performance or applications of the 6x19 fully locked coil wire rope, or need detailed technical parameters and a quotation, please contact us at any time. Kindly provide your specific requirements (such as diameter, core type, surface treatment, length, etc.), and we will provide a customized solution.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

简体中文
English