LM Stainless Steel Wire Rope GB1X19 (12/6/1)

LM Stainless Steel Wire Rope GB1X19 (12/6/1)

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Product Details 

1x19 stainless steel wire rope is a common stainless steel wire rope construction. With its attractive appearance, high breaking load and low elongation, 1x19 is widely used throughout the marine, mining, construction and other industries.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy GB Compacted Stainless Steel Wire Rope 1X19 (12/6/1)

Engineering Applications 

  • Railings

  • Fixed rigging

  • Mast stays

  • Guardrails

  • Structural components

  • Guy wires

  • Marine engineering

  • Wastewater treatment engineering

Breaking load

Diameter

Weight

Minimum breaking load (1570 MPa)

Minimum breaking load (1570 MPa)

mm

kg/m

KN

Kg

40.0914.51479
50.1423.92438
60.234.83550
70.2748.24916
80.3560.36151
90.4473.57497
100.5595.89772
110.6611011220
120.7914114382

General engineering wire rope

 Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also provide high-quality special wire ropes.

Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and abrasion. All our wire ropes are designed to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and comply with ISO9001.


Selection Guide

When selecting, first confirm the load requirements of the application, the corrosive environment and the structural connection method, then determine the wire rope diameter, construction (such as 1x19, 7x7, 6x19, etc.) and surface treatment (bright or galvanized) accordingly. Different diameters and constructions correspond to different minimum breaking loads; it is recommended to base the choice on actual working conditions. Please contact us for detailed specifications and quotations, and we can assist you with the selection.

Product Advantages

Greenlogy TEC (LM) stainless steel wire rope adopts a 1x19 construction, offering high breaking load and low elongation, making it suitable for fixed rigging and structural support requiring high dimensional stability. Products can be supplied with bright or galvanized surface treatment as needed, balancing corrosion resistance and appearance requirements. Drawing on Greenlogy TEC's supply experience in the wire rope field, we can provide multi-specification standard products as well as special wire rope options.

Inquiry Guidance

For specific diameters, constructions, surface finishes, or bulk supply solutions, please contact us for detailed specifications and quotations. Kindly provide information such as your application, required diameter, and quantity so that we can recommend suitable products for you. We look forward to communicating with you and supporting your project requirements.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor