LM Wire Rope GB1x19
Request a Quote
Please feel freely to contact with us for new price .
Product Details
1x19 wire rope is one of the common wire rope constructions. 1x19 offers excellent breaking strength and tensile performance. It has a neat appearance. It is widely used in the marine industry, mining, construction and other fields.
Surface treatment: bright or galvanized
Standard: GB/T20118-2006

Engineering Applications
Railings
Fixed rigging
Mast stays
Guardrails
Structural components
Guy wires
Marine engineering
Wastewater treatment engineering
Breaking load
Diameter
| Weight
|
Minimum breaking load (1570 MPa)
|
Minimum breaking load (1570 MPa)
|
|---|---|---|---|
mm | kg/m | KN |
Kg |
| 2 | 0.02 | 3.14 | 320 |
| 2.5 | 0.03 | 4.9 | 499 |
| 3 | 0.04 | 7.06 | 719 |
| 4 | 0.08 | 12.6 | 1284 |
| 5 | 0.12 | 19.6 | 1998 |
| 6 | 0.18 | 28.2 | 2875 |
| 7 | 0.24 | 34.8 | 3548 |
| 8 | 0.31 | 45.5 | 4639 |
| 9 | 0.4 | 57.6 | 5873 |
| 10 | 0.49 | 71.1 | 7250 |
| 11 | 0.59 | 86 | 8769 |
| 12 | 0.7 | 102 | 10401 |
| 14 | 0.96 | 139 | 14174 |
| 16 | 1.25 | 182 | 18558 |
| 19 | 1.76 | 212 | 21617 |
| 22 | 2.36 | 285 | 29061 |
| 26 | 3.3 | 398 | 40584 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm and include 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high level of performance to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customized services; our team of engineers can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
When selecting 1x19 wire rope, it is recommended to determine the appropriate diameter and surface treatment based on the load requirements of the actual project, the operating environment (such as whether galvanized corrosion protection is needed) and the specifications of the matching rigging. For the weight and minimum breaking load corresponding to different diameters, please refer to the table above. If you need selection advice for specific working conditions, please contact us for detailed specifications and quotations.
Product Advantages
1x19 construction wire rope offers high breaking strength and good tensile performance, with a neat appearance. Bright or galvanized treatment can adapt to different corrosive environments. Greenlogy TEC (LM) supplies multi-strand bright or galvanized wire rope, with diameters ranging from 0.5 mm to 64 mm, meeting the diverse needs of the marine, mining, construction and other fields.
Inquiry Guidance
For detailed specifications, surface treatment options, packaging methods, and bulk purchasing of 1x19 wire rope, please contact us to obtain detailed specifications and a quotation. Please provide the required diameter, quantity, and application, and we will provide support as soon as possible.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.