Structural Profiles - Curved Flat Bar (Orthophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
FRP pultruded profiles are made from glass fiber reinforcement as the raw material, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Corner Radius | Width × Thickness | Width × Thickness | ||
| FS50A | 50*3.2 | 0.29 | 2" x 1/8" | 0.64 |
| FS60A | 60*3.2 | 0.36 | 19/8" x 1/8" | 0.79 |
| FS70 | 70*4 | 0.54 | 19" x 3/16" | 1.19 |
| FS90A | 90*3.2 | 0.54 | 7/2" x 1/8" | 1.19 |
| FS100 | 100*3.2 | 0.6 | 4" x 1/8" | 1.32 |
| FS120 | 120*3 | 0.7 | 19/4" x 1/8" | 1.54 |
Application fields

Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistant
Low maintenance
Flame retardant
Low installation cost
Heavy metal resistant
Long service life
Non-conductive and non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type: economical with good performance, moderate resistance to acid, alkali and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and non-conductive properties. Where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles deliver years of low-maintenance operation. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC Profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, Longitudinal | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, Transverse | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, Longitudinal | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, Transverse | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, Longitudinal | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, Transverse | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, Longitudinal | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, Transverse | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, Longitudinal | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, Transverse | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, Longitudinal | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, Transverse | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Elastic Modulus | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punching Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact, Longitudinal (LW) | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact, Transverse (CW) | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Maximum value % | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, longitudinal (LW) | D-696 | 10^-6in./in./℃ | 8 |
Flammability performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = longitudinal, CW = transverse, PF = perpendicular to the laminate surface
*Applicable to ISOFR and VEFR only
Applications
Curved flat bars are commonly used in structural parts that require a curved profile or edge reinforcement, such as platform handrails, walkway frames, equipment supports and decorative trim. Their orthophthalic resin system suits general industrial and outdoor environments; weathering and corrosion resistance should be assessed against actual service conditions. Contact us for detailed recommendations.
Selection Guide
When selecting, consider the arc radius, cross-section dimensions, load requirements and installation method to ensure compatibility with adjacent components. You may provide drawings or service conditions, and our technical team will help recommend suitable specifications. Contact us for detailed specifications and quotations.
Product Advantages
This profile is made from glass fiber reinforcement and an orthophthalic resin system through a pultrusion process. It offers light weight, high strength, corrosion resistance and electrical insulation, and its curved design facilitates streamlined structures. Compared with traditional metal materials, it is easier to cut and install, helping to reduce long-term maintenance costs.
Inquiry
For stock availability, pricing or customization options for Structural Profiles - Curved Flat Bar (Orthophthalic), please contact us. Kindly provide the required specifications, quantity and application, and we will respond promptly with a detailed quotation and technical support.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English