Structural Profiles - Flat Panel (Vinyl Ester)
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and then pulled out by a pulling machine. As a new type of composite material with good physical properties, they are widely used in high-strength and long-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Flat | Thickness × Width | Thickness × Width | ||
FP32A | 3.2*1000 | 6.18 | 1/8" x 39" | 13.6 |
FP32B | 3.2*1220 | 7.42 | 1/8" x 48" | 16.4 |
FP40A | 4*800 | 6.2 | 3/16" x 32" | 13.7 |
FP40B | 4*1200 | 9.19 | 3/16" x 48" | 20.3 |
FP48 | 4.8*1000 | 9.3 | 3/16" x 39" | 20.5 |
FP50A | 5*440 | 4.25 | 3/16" x 17" | 9.37 |
FP50B | 5*1220 | 11.8 | 3/16" x 48" | 26 |
FP64 | 6.4*1220 | 14.84 | 1/4" x 48" | 32.7 |
FP95 | 9.5*1220 | 22.02 | 3/8" x 48" | 48.6 |
FP127 | 12.7*1220 | 29.44 | 1/2" x 48" | 64.9 |
FP160 | 16*1220 | 37.2 | 5/8" x 48" | 82 |
FP190 | 19*1220 | 44.1 | 3/4" x 48" | 97.2 |
FP254 | 25.4*1220 | 59 | 1" x 48" | 130 |
Markets

Construction
Bridges and Highways
Chemical
Food and Beverage
Manufacturing
Metals and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion-resistant
Low maintenance
Flame-retardant
Low installation cost
Heavy-metal-free and safe
Long service life
Non-conductive and non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame-retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | An economical VEFR-type product with good performance and moderate resistance to acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Where steel, aluminum or timber members have traditionally been specified, durable Greenlogy TEC profiles provide years of low-maintenance service. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC Profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, Lengthwise | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, Crosswise | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, Lengthwise | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, Crosswise | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, Lengthwise | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, Crosswise | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, Lengthwise | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, Crosswise | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, Lengthwise | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, Crosswise | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, Lengthwise | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, Crosswise | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-Beam Shear Strength | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear Strength | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact Strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact Strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | 25 max |
Combustibility* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = longitudinal, CW = transverse, PF = perpendicular to the laminate surface
*Applicable to ISOFR and VEFR only
Applications
This structural profile – flat sheet is suitable for platforms, walkways, handrails, support beams and various load-bearing structural components where strength, span and corrosion resistance are required. It can also serve as a structural alternative in corrosive environments such as chemical processing, marine and wastewater treatment. For load and span matching in specific applications, please contact us to discuss your actual working conditions.
Selection guide
When selecting, first confirm the thickness and width specifications, then evaluate the required cross-section dimensions based on the load, span and corrosion conditions of the service environment. The specifications listed in the table cover common flat sheet sizes. If the existing specifications do not fully match your needs, please contact us for detailed specifications and selection advice.
Product advantages
Made from glass fiber reinforcement with a resin matrix through a pultrusion process, it offers good physical properties and corrosion resistance, making it suitable for high-strength, long-span applications and for situations where conventional materials are prone to corrosion. Compared with metal materials, it is lighter in weight, which facilitates transport and installation. For specific performance parameters, please contact us for detailed information.
Inquiry
For detailed specifications, pricing, supply capability and other commercial terms of this structural profile – flat sheet, please contact us for detailed specifications and a quotation. Our team will provide support according to your application requirements.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English