FRP pultruded profiles are a new type of composite material made from glass fiber reinforcement as the raw material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after full impregnation, the material is heated, formed, and cured in a metal mold and then drawn by a pulling machine. With good physical properties, they are widely used in high-strength and long-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Hook plate | A*B*T | A*B*T | ||
| 9*70*3.2 (beveled edge) | 0.48 | 1" x 1" x 1/8" (beveled edge) | 1.06 | |
| 25*60*3 | 0.5 | 1" x 19/8" x 1/8" | 1.1 | |
| 25*50*3(75°) | 0.45 | 1" x 2" x 1/8" (75°) | 0.99 | |
| 30*70*4(90°) | 0.75 | 19/16" x 11/4" x 3/16" (90°) | 1.65 | |
| 30*70*3.2(90°) | 0.7 | 19/16" x 11/4" x 1/8" (90°) | 1.54 | |
| 30*90*3(87°) | 0.72 | 19/16" x 7/2" x 1/8" (87°) | 1.59 | |
| 38*230*3.2(87°) | 1.65 | 3/2" x 9" x 1/8" (87°) | 3.64 | |
| 40*254*6.4(87°) | 3.55 | 25/16" x 10" x 1/4" (87°) | 7.83 | |
| 50*140*3.2(87°) | 1.19 | 2" x 11/2" x 1/8" (87°) | 2.62 | |
| 55*152*3.6(87°) | 1.55 | 9/4" x 6" x 1/8" (87°) | 3.42 | |
| 55*230*3.6(87°) | 2.14 | 9/4" x 9" x 1/8" (87°) | 4.72 | |
| 55*205*3.2(87°) | 1.62 | 9/4" x 8" x 1/8" (87°) | 3.57 | |
| 55*55*3.2(87°) | 0.8 | 9/4" x 9/4" x 1/8" (87°) | 1.76 | |
| 55*70*3.2(87°) | 0.9 | 9/4" x 11/4" x 1/8" (87°) | 1.98 | |
| 30*76*3 | 0.6 | 19/16" x 3" x 1/8" | 1.32 | |
| 30*76*4 | 0.8 | 19/16" x 3" x 3/16" | 1.76 | |
| 25*50*3.2(90°) | 0.45 | 1" x 2" x 1/8" (90°) | 0.99 | |
| 25*50*4(90°) | 0.51 | 1" x 2" x 3/16" (90°) | 1.12 | |
| 25*100*3.2(87°) | 0.75 | 1" x 4" x 1/8" (87°) | 1.65 | |
| Rounded corner | 30*75*3.5 | 0.69 | 19/16" x 3" x 1/8" | 1.52 |
| Rounded corner | 30*100*3.2 | 0.8 | 19/16" x 4" x 1/8" | 1.76 |
| Right angle | 30*100*3.2 | 0.85 | 19/16" x 4" x 1/8" | 1.87 |
| 30*152*3.2 | 1.2 | 19/16" x 6" x 1/8" | 2.65 | |
| Rounded corner | 30*230*3.2 | 1.6 | 19/16" x 9" x 1/8" | 3.53 |
| Right angle | 30*230*3.2 | 1.7 | 19/16" x 9" x 1/8" | 3.75 |
| 55*300*4(90°) | 2.8 | 9/4" x 12" x 3/16" (90°) | 6.17 | |
| 55*345*4(87°) | 3.25 | 9/4" x 27/2" x 3/16" (87°) | 7.17 | |
| 30*381*3.2(87°) | 2.7 | 19/16" x 15" x 1/8" (87°) | 5.95 | |
| 55*400*3.2 | 2.8 | 9/4" x 63/4" x 1/8" | 6.17 |
Markets

Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Entertainment and leisure
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Heavy-metal safety
Long service life
Electrical and thermal insulation
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Harsh acid, alkali and other corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type, economical, with good resistance to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles (manufactured by Greenlogy TEC) are widely used in many fields, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC Profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, longitudinal | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, transverse | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, longitudinal | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, transverse | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, longitudinal | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, transverse | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, longitudinal | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, transverse | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, longitudinal | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched cantilever beam impact, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched cantilever beam impact, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max 25 |
Flammability performance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies only to ISOFR and VEFR
Applications
Hook plates (isophthalic) are commonly used for edge fixing on platforms in chemical, electroplating and wastewater treatment applications, connecting to grating, handrails or profiles to provide reliable support and fastening. In applications requiring high strength and corrosion resistance, such as marine engineering and oil platforms, they also offer performance advantages. Actual suitability should be assessed against specific operating conditions; contact us for application guidance.
Selection guide
When selecting, determine the hook plate dimensions (A*B*T), angle (e.g. 75° or beveled edge) and installation method to ensure compatibility with the existing structure. Isophthalic resin gives the product better corrosion resistance than orthophthalic resin, making it suitable for more demanding chemical environments. For detailed specifications and selection support, please contact us for professional advice.
Product advantages
Made with isophthalic resin, hook plates offer excellent corrosion resistance and mechanical strength, are lightweight, easy to install, and are insulating and non-magnetic. Glass fiber reinforcement ensures long-term durability, suitable for high-load and outdoor environments. We can provide customized solutions to meet your requirements; please contact us.
Inquiry
Contact us for detailed specifications, technical parameters and quotations. We provide professional selection support and customization services to meet your project requirements. Please contact us via our website or email, and we will reply as soon as possible.
Operating environment
- Suitable for a wide range of indoor and outdoor environments; the glass fiber reinforced isophthalic resin system keeps hook plate performance stable in humid, salt-fog and general chemical corrosive atmospheres.
- Can be used long-term from ambient to moderate temperatures for platforms, walkways and structural support applications with heat resistance requirements; ambient temperature fluctuations have little effect on the dimensional stability of the profiles.
- Good resistance to acids, alkalis, salts and industrial atmospheres, suitable for hook plate connections and fixing in corrosive environments such as chemical plants, wastewater treatment and marine platforms.
- Under outdoor conditions with UV exposure, use with surface protection measures is recommended to extend the service life of the hook plates and their connecting structures.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English