FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed, and cured in a metal mold and then pultruded by a pulling machine. They have good physical properties and are widely used in high-strength, large-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in)
| Weight (lbs/in) |
|---|---|---|---|---|
I-beam | A*B*T1*T2 | A*B*T1*T2 | ||
| IB32 | 15*32*6.4*4 | 0.51 | 0.59*1.26*0.25*0.16 | 1.12 |
| IB38A | 30*38*3*3 | 0.53 | 1.18*1.5*0.12*0.12 | 1.17 |
| IB45A | 45*9*180*12 | 5.4 | 1.77*0.35*7.09*0.47 | 11.9 |
| IB50A | 50*102*6.4*6.4 | 2.4 | 1.97*4.02*0.25*0.25 | 5.29 |
| IB50B | 50*102*8*8 | 3 | 1.97*4.02*0.31*0.31 | 6.61 |
| IB76A | 76*152*6.4*6.4 | 3.59 | 2.99*5.98*0.25*0.25 | 7.91 |
| IB76B | 76*152*9.5*9.5 | 5.32 | 2.99*5.98*0.37*0.37 | 11.73 |
| IB102A | 102*203*9.5*9.5 | 7.2 | 4.02*7.99*0.37*0.37 | 15.87 |
| IB102B | 102*203*12.7*12.7 | 9.5 | 4.02*7.99*0.5*0.5 | 20.94 |
| IB120 | 120*240*12*12 | 10.5 | 4.02*9.45*0.47*0.47 | 23.15 |
| IB127A | 127*254*9.5*9.5 | 9 | 5*10*0.37*0.37 | 19.84 |
| IB127B | 127*254*12.7*12.7 | 11.9 | 5*10*0.5*0.5 | 26.24 |
| IB127C | 127*152*9.5*9.5 | 7.1 | 5*5.98*0.37*0.37 | 15.65 |
| IN127D | 127*152*12.7*12.7 | 9.2 | 5*5.98*0.5*0.5 | 20.28 |
| IB152A | 152*305*9.5*9.5 | 10.7 | 5.98*12.01*0.37*0.37 | 23.68 |
| IB152B | 152*305*12.7*12.7 | 14.3 | 5.98*12.01*0.5*0.5 | 31.53 |
Application Markets

Construction
Bridges & Highways
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gas
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Resistant to heavy metals
Long service life
Non-conductive, non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Standard colors | Recommended applications |
|---|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Grass green, yellow, gray, orange | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | Grass green, yellow, gray | VEFR type, economical, with good performance and moderate resistance to acid, alkali and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | Grass green, yellow, gray | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are widely used in various scenarios, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. In areas where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles can provide years of low-maintenance service. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.
Greenlogy TEC Profiles
Mechanical Properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear strength | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear strength | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round bars and square bars
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | Maximum percentage | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volt/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Applications
Structural profiles – I-beams are suitable for load-bearing and support locations requiring strength and span, such as platform walkways, trestles, equipment supports, handrail framing and structural frames in corrosive environments. Different resin systems and fiber lay-ups can be adapted to various service conditions; contact us for detailed specifications and a quotation.
Selection guidance
Selection should take into account load type, span, support conditions, service environment and connection method, on which basis section size and lengthwise requirements are determined. As service conditions vary considerably, we recommend providing your operating conditions so that we can help confirm a suitable model; contact us for detailed specifications and a quotation.
Product advantages
FRP I-beams are made from glass fiber reinforcement combined with resin, offering light weight and high strength, corrosion resistance, electrical insulation and non-magnetic properties, and ease of cutting and on-site fabrication, making them convenient substitutes where metal profiles tend to corrode. Specific performance varies with formulation and specification; contact us for detailed specifications and a quotation.
Inquiry guidance
To confirm section specifications, length, color, resin type or a matching connection solution, please provide drawings or service conditions and we will make recommendations accordingly. Contact us for detailed specifications and a quotation, and we can also discuss samples and bulk supply further.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English