FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the outer reinforcement layer. After being fully impregnated, the material is heated, formed and cured in a metal die and pulled by a pultrusion machine to produce a new type of composite material with good physical properties, widely used in high-strength and long-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
| Kick plate | A*B*T | A*B*T | ||
| M2 | 100*13*3.2 M型 | 1.1 | 3.94*0.51*0.13 M型 | 2.43 |
| M3 | 100*16*5 M型 | 1.3 | 3.94*0.63*0.2 M型 | 2.87 |
| M4 | 148*12*3 M型 | 1.27 | 5.83*0.47*0.12 M型 | 2.8 |
| W1 | 100*19*5 W型 | 1.36 | 3.94*0.75*0.2 W型 | 3 |
| W2 | 100*15*3.2 W型 | 1.1 | 3.94*0.59*0.13 W型 | 2.43 |
| W3 | 150*15*3.2 W型 | 1.6 | 5.91*0.59*0.13 W型 | 3.53 |

Construction
Bridges and highways
Chemical
Food and beverage
Manufacturing
Metals and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation and entertainment
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance cost
Flame retardant
Low installation cost
Heavy-metal protection and safety
Long service life
Non-conductive and non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin type
Code | Resin type | Flame retardancy | Standard color | Recommended applications |
|---|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Grass green, yellow, gray, orange | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | Grass green, yellow, gray | Vinyl ester type is economical with good performance, moderate resistance to acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | Grass green, yellow, gray | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles deliver years of low-maintenance service in areas where steel, aluminum or timber members are traditionally specified. Today these profiles are often used in highly corrosive applications that would otherwise require stainless steel and other costly components.
Flame retardancy | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flame retardancy* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, longitudinal | D-495 | 秒(s) | 120 |
Dielectric strength, longitudinal | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | V/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate face
*Applies to ISOFR and VEFR only
Applications
Structural profiles - kick plates are commonly used in chemical platforms, wastewater treatment, marine engineering and power facilities and other corrosive environments, serving as edge protection and toe-board components, used together with FRP grating and pultruded profiles. To confirm suitability for your specific operating conditions, please contact us for detailed specifications and a quotation.
Selection guide
During selection, you can make an initial match from the A*B*T specifications based on the dimensions of the mounting surface, the required cross-sectional shape (such as M-shape) and load-bearing requirements. As specific parameters and customization needs are involved, we recommend providing drawings or operating conditions so that we can help recommend a suitable model. Please contact us for detailed specifications and a quotation.
Product advantages
This kick plate is pultruded from glass fiber reinforcement and resin, featuring corrosion resistance, light weight and high strength, electrical insulation, and ease of cutting and installation, making it suitable for high-humidity and chemical media environments. Different resin systems can meet various operating conditions. Please contact us for detailed specifications and a quotation.
Inquiry guidance
To learn about the available specifications, surface treatments and bulk supply information for structural profiles - kick plates, please provide us with your dimensions, quantity and operating environment. Please contact us for detailed specifications and a quotation; we will provide a targeted solution based on your requirements.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English