FRP pultruded structural profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer; after full impregnation, they are heated, formed and cured in a metal mold and pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.
.png?access_token=fe26106f-1237-434c-93f7-f44049242e94)
Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
Toe Board | A*B*T | A*B*T | ||
M2 | 100*13*3.2 M型 | 1.1 | 4" x 1/2" x 1/8" M型
| 2.43 |
M3 | 100*16*5 M型 | 1.3 | 4" x 5/8" x 3/16" M型 | 2.87 |
M4 | 148*12*3 M型 | 1.27 | 23/4" x 1/2" x 1/8" M型 | 2.8 |
W1 | 100*19*5 W型 | 1.36 | 4" x 3/4" x 3/16" W型 | 3 |
W2 | 100*15*3.2 W型 | 1.1 | 4" x 9/16" x 1/8" W型 | 2.43 |
W3 | 150*15*3.2 W型 | 1.6 | 6" x 9/16" x 1/8" W型 | 3.53 |
Market

Construction
Bridge and highway
Chemical
Food and beverage
Manufacturing
Metal and mining
Microelectronics
Oil and gas
Pharmaceutical
Power
Pulp and paper
Recreation and entertainment
Telecommunications
Transportation
Water and wastewater treatment
Features:
Corrosion resistance
Low maintenance cost
Flame retardant
Low installation cost
Resistant to heavy metal hazards
Long service life
Electrical and thermal insulation
High specific strength
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | An economical VEFR-type product with good performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles from Greenlogy TEC are used across a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. In areas where steel, aluminum or wood components have traditionally been specified, durable Greenlogy TEC profiles provide years of low-maintenance service. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile Stress, Lengthwise | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, Crosswise | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, Lengthwise | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, Crosswise | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, Lengthwise | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, Crosswise | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, Lengthwise | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, Crosswise | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, Lengthwise | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, Crosswise | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, Lengthwise | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, Crosswise | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact, Lengthwise | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact, Crosswise | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical Properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flammability* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | V/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Application Scenarios
This isophthalic structural profile toe board is suitable for platform, walkway, tank farm and trench edge protection where corrosion resistance and load-bearing are required, providing protection, edge sealing and a finished appearance. It is commonly used with FRP grating or profiles in chemical, wastewater treatment, electroplating, marine engineering and similar environments. For specific environmental suitability, please contact us for detailed specifications and a quotation.
Selection Guide
During selection, the cross-section dimensions A*B*T and models such as M2, M3 and M4 can be determined based on the span, load and fixing method at the installation location. The isophthalic resin system is suitable for highly corrosive working conditions. If it is to be used with other FRP profiles or grating, we recommend providing drawings or on-site dimensions. For detailed specifications and a quotation, please contact us.
Product Advantages
Using glass fiber reinforcement and isophthalic resin as the matrix, it is formed through heating, molding, curing and pultrusion, offering good mechanical properties, corrosion resistance and dimensional stability, and is suitable for high-strength, long-span applications. Different surface treatments can be selected according to requirements, making installation and maintenance easier. Please contact us for detailed specifications and a quotation.
Inquiry Guide
To confirm the dimensions, color, length and matching scheme of this isophthalic toe board, please share your application scenario and required quantity with us, and we will provide detailed specifications and a quotation. You may also contact us for samples and technical support.
Operating Environment
- This isophthalic resin toe board is a pultruded FRP structural profile, so it is suitable for both indoor and outdoor installation, for protecting wall bases, platform edges or walkway edges.
- The isophthalic polyester resin system gives this profile better resistance to moisture and to splashes and spills of mild chemical media than standard orthophthalic resin, making it a practical choice for wet process areas, washdown areas and coastal or humid locations.
- As a glass fiber reinforced composite, this toe board does not corrode like steel and does not require painting, so it maintains its function in wet, salt-laden or mildly corrosive environments.
- Continuous service temperature and resistance to specific chemicals depend on the resin, the medium and the concentration involved; please share your on-site conditions with us, and we will confirm whether this isophthalic profile is the right grade for your project.