Structural Profiles - Seven-Hole Hollow Board (Orthophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
FRP profiles are made from glass fiber reinforcing material, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold, and pultruded under the pull of a traction machine. This new composite material has good physical properties and is widely used in high-strength, long-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
| 600*8.5*56*8 | 25.4 | 24" x 5/16" x 2" x 5/16" | 56 |
Markets

Construction
Bridges and Highways
Chemical
Food and Beverage
Manufacturing
Metals and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion resistant
Low maintenance cost
Flame retardant
Low installation cost
Heavy metal resistant
Long service life
Non-conductive and non-thermally-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | A VEFR economical grade with excellent performance, resistant to moderate acids, alkalis and solvents |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Application scope:
Greenlogy TEC pultruded FRP structural profiles from Greenlogy TEC cover a wide range of applications and combine corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max. 25 |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Applications
As a structural profile, the seven-hole hollow profile is suitable for market sectors such as construction, bridges and highways, chemicals, food and beverage, manufacturing, metals and mining, and microelectronics, and can be used for platforms, walkways, support structures, and similar applications. When selecting for a specific scenario, load and environmental conditions must be taken into account; you are welcome to contact us for detailed application advice.
Selection Guidance
During selection, factors such as load requirements, span, support conditions, corrosive environment, and installation method must be considered. We recommend providing operating parameters so that our technical team can assist in recommending suitable specifications. You are welcome to contact us for detailed selection support.
Product Advantages
This profile is made of glass fiber reinforced material and a resin matrix, formed through the pultrusion process. It features light weight, high strength, corrosion resistance, and electrical insulation, and is suitable for high-strength, long-span applications. Compared with traditional materials, it can extend service life and reduce maintenance costs under specific environments.
Inquiry Guidance
For information such as detailed specifications, dimensions, weight, price, minimum order quantity, and delivery time, you are welcome to contact us. Please provide your specific requirements, and we will reply as soon as possible and provide professional support.
Operating Environment
- This seven-hole hollow profile is made of glass fiber reinforced material, with resin as the binder and a glass fiber cloth wrapping reinforcement layer, and is suitable for indoor and outdoor installation environments where moisture and atmospheric exposure exist.
- Because the pultruded structure combines glass fiber reinforced material with resin, this profile is used in environments where corrosive media and humidity are common, such as chemicals, food and beverage, manufacturing, metals and mining, and microelectronics.
- The hollow seven-hole cross-section reduces weight while maintaining structural rigidity, so this profile is selected for high-strength, long-span applications in construction, bridges and highways, and industrial environments.
- For specific temperature ranges, chemical corrosion resistance grades, and other operating conditions, please contact Greenlogy TEC and provide your application details.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.