Structural Profiles - Seven-Hole Partition Panel (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Nantong Greenlogy TEC Electronic Technology Co., Ltd.
FRP profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the covering reinforcement layer. After thorough impregnation, they are heated, formed and cured in metal molds, then pultruded by a pulling machine. This new composite material offers good physical properties and is widely used in high-strength, long-span applications.

Grade | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
| 1000*140*5 | 31.6 | 39" x 11/2" x 3/16" | 69.7 |
Markets

Construction
Bridges and Highways
Chemical
Food and Beverage
Manufacturing
Metals and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion resistance
Low maintenance cost
Flame retardant
Low installation cost
Safe in heavy-metal environments
Long service life
Non-conductive and non-thermal-conductive
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Severe acid, alkali and other corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | An economical VEFR type with good, moderate acid, alkali and solvent resistance |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP structural profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with non-thermal-conductive and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, longitudinal | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, transverse | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, longitudinal | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, transverse | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, longitudinal | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, transverse | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, longitudinal | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, transverse | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, longitudinal | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, transverse | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, longitudinal | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, transverse | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Izod notched impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Izod notched impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | Max 25 |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies only to ISOFR and VEFR
Application Scenarios
The seven-hole partition wall board (isophthalic) is suitable for partition walls, platforms, walkways and equipment enclosures that require both corrosion resistance and structural strength, and is commonly found in corrosive environments such as chemical, food, electroplating and water treatment facilities. The isophthalic resin system performs stably in resistance to chemical media and damp heat, making it suitable for areas exposed long-term to humid or mildly acidic/alkaline atmospheres. For specific application suitability, please contact us to confirm based on your site conditions.
Selection Guidance
When selecting, take into account the medium type and concentration in the service environment, long-term working temperature, span and load conditions, and the installation and fixing method. The seven-hole structure reduces self-weight while maintaining the section moment of inertia, making it suitable for partition applications that are weight-sensitive or require large spans. As this catalog entry does not list complete mechanical and corrosion-resistance data, please contact us for detailed specifications and selection support.
Product Advantages
This profile uses fiberglass reinforcement with an isophthalic resin matrix, formed by the pultrusion process, and offers the typical composite characteristics of light weight, high strength, corrosion resistance, non-conductivity and low maintenance. The seven-hole cross-section increases stiffness for the same material usage, is easy to cut and install on site, and can reduce the frequency of later maintenance and replacement. Actual performance is subject to testing and the technical agreement of the order.
Inquiry Guidance
For information on dimensional tolerances, color, surface treatment, packaging and bulk supply solutions, please contact us for detailed specifications and a quotation. Please provide details such as the service environment, span, load and quantity, and we will recommend suitable specifications and arrange technical follow-up accordingly.
Service Environment
- A structural profile made from glass fiber reinforcement bonded with pultruded resin, suitable for normal use in indoor factories, outdoor structures and semi-enclosed industrial areas where temperature and humidity fluctuate with the seasons.
- The molded cured surface of these FRP structural profiles resists moisture and the corrosive splashes, vapors and chemically laden air found in chemical, food and beverage, metal and mining processing environments, so the profiles require no paint protection.
- Because the glass fiber cloth reinforcement layers are fully impregnated with resin, the profiles retain their shape and load-bearing function in high-strength, long-span installations such as partition frames and support structures exposed to washdown or humid process areas.
- For use in a specific medium or at a specified temperature or humidity level, please provide your project conditions and contact us so that the profile selection can be confirmed against the full parameter table; no universal usage limitation applies.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文