FRP profiles are a new type of composite material made from glass fiber reinforced material, with resin as the binder and glass fiber cloth as the covering reinforcement layer. After full impregnation, they are heated, formed, and cured in a metal mold and then pulled by a pultrusion machine. They have good physical properties and are widely used in high-strength and large-span applications.

Type | Size (mm) | Weight (kg/m) | Size (in) | Weight (lbs/in) |
|---|---|---|---|---|
U-shaped Square Tube Handrail Profile | A*B*T | A*B*T | ||
| 62*59*4.5 | 1.5 | 5/2" x 9/4" x 3/16" | 3.31 | |
| 62*60*5 | 1.7 | 5/2" x 19/8" x 3/16" | 3.75 |
Market

Construction
Bridge and Highway
Chemical
Food and Beverage
Manufacturing
Metal and Mining
Microelectronics
Oil and Gas
Pharmaceutical
Power
Pulp and Paper
Recreation
Telecommunications
Transportation
Water and Wastewater Treatment
Features:
Corrosion resistance
Low maintenance
Flame retardant
Low installation cost
Suitable for heavy-metal environments
Long service life
Electrical and thermal insulation
High strength-to-weight ratio
Raw material introduction — resin types
Code | Resin type | Flame retardant performance | Recommended applications |
|---|---|---|---|
VEFR-25 | Vinyl ester type | Oxygen index 28 and above | Acid, alkali and other harsh corrosive environments |
IFR-25 | Isophthalic type | Oxygen index 28 and above | VEFR type, economy grade, with good, moderate acid/alkali and solvent resistance |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
Applications:
Greenlogy TEC pultruded FRP profiles are used in a wide range of applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation. Durable Greenlogy TEC profiles provide years of low-maintenance service where steel, aluminum or wood components are traditionally used. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.
Greenlogy TEC profiles
Mechanical properties | ASTM | Unit | Value | Unit | Value |
|---|---|---|---|---|---|
Tensile stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of elasticity | Full section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short-beam shear strength | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch shear strength | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod impact strength, LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod impact strength, CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excluding round rods and square rods
Physical properties | ASTM | Unit | Value |
|---|---|---|---|
Barcol hardness | D-495 | --- | 45 |
24-hour water absorption | D-570 | % max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of thermal expansion, LW | D-696 | 10^-6in./in./℃ | 8 |
Flame retardant performance | ASTM | Unit | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame spread | 25 max |
Flame resistance* | D-635 | --- | Non-combustible |
Electrical properties | ASTM | Unit | Value |
|---|---|---|---|
Arc resistance, LW | D-495 | 秒(s) | 120 |
Dielectric strength, LW | D-149 | kv./in. | 35 |
Dielectric strength, PF | D-149 | Volts/mil | 200 |
Dielectric constant, PF | D-150 | @60hz | 5 |
LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface
*Applies to ISOFR and VEFR only
Application Scenarios
The structural profile — U-shaped square tube handrail profile (isophthalic) — is commonly used for platform railings, stair handrails, walkway enclosures, bridge pedestrian passages and other locations requiring both load-bearing capacity and protection. The isophthalic resin system gives it good resistance in humid, mildly corrosive or outdoor environments, making it suitable for applications with long-term service stability requirements. Please confirm specific service conditions with us based on actual loads and media.
Selection Guidance
When selecting, first define the required cross-section dimensions, wall thickness and span of the handrail, then determine the matching fittings based on the installation method and connection joints. Different specifications differ in self-weight and rigidity; larger spans or higher protection requirements generally require larger cross-sections or additional support. To verify specifications against project conditions, please contact us for detailed specifications and a quotation.
Product Advantages
This profile is pultruded from glass fiber reinforcement and isophthalic resin, combining light weight, high strength and corrosion resistance; it is also non-conductive and non-magnetic, making it suitable for long-term use in a variety of environments. Its surface is dense and requires little routine maintenance, making it suitable as a substitute for some traditional metal handrail materials. For comparative information on different cross-sections and performance, please contact us for further details.
Inquiry Guidance
To confirm specifications, color, length and the selection of matching connectors, please provide drawings or service conditions and our technical team will assist with verification. You are welcome to contact us for detailed specifications and a quotation, and to discuss sample and bulk supply arrangements.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English