Greenlogy TEC
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




20*20*30(mm)
Panel size available:
1007*4047,1007*3007 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:20
Open Aera:42%
Approx Weight:18kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating is commonly used in platforms, walkways and trench covers with high corrosion resistance requirements in electroplating, chemical, wastewater treatment and marine engineering, and is also suitable for maintenance access ways requiring insulation and lightweight load-bearing. The 20×20H30 mesh size suits areas with combined requirements on open area and load capacity. Welcome to contact us to describe your working conditions for suitable recommendations.
Selection Guide
When selecting, it is usually necessary to confirm the resin system (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.), grating thickness and mesh size, load rating, and the corrosive media and temperature conditions of the service environment. The raw material formulation and resin type listed on this page are for reference only; please confirm specific specifications with us. Welcome to contact us for detailed specifications and a quotation.
Product Advantages
FRP molded grating is integrally molded from glass fiber reinforced resin, featuring corrosion resistance, lightweight and high strength, insulation and non-magnetic properties, and ease of cutting and installation, with relatively low long-term maintenance costs. Different resin systems can correspond to different corrosion-resistance and flame-retardant requirements; specific performance needs to be evaluated based on actual working conditions. Welcome to contact us for detailed specifications and a quotation.
Inquiry Guidance
To learn about the dimensional tolerances, colors, surface treatments, packaging and transportation details of FRP Grating 20×20H30, please provide information such as the application scenario, quantity and target market so that we can offer a targeted solution. Welcome to contact us for detailed specifications and a quotation, and we will arrange a dedicated contact as soon as possible.
Operating Environment
- This molded FRP grating uses unsaturated polyester resin—including isophthalic, bisphenol, and phenolic types—as its matrix, allowing it to serve in indoor and outdoor installations where moisture and chemical exposure are routine.
- The phenolic resin option provides high flame retardancy with an oxygen index of about 80, making this FRP grating suitable for fire-sensitive industrial environments where low toxicity and fire safety are priorities.
- With E-glass fiber reinforcement and ATH or PR fillers, the grating handles corrosive media commonly found in chemical processing, wastewater treatment, and marine/offshore walkways and platforms.
- Contact us for the full parameter list and to confirm the resin grade and configuration that match your specific operating conditions.