FRP Molded Grating 20*20H14
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




20*20*14(mm)
Panel size available:
1247*4047,1007*3007 Bidirectional force.
Bearing bar thickness (Top/Bottom):7.5/5.0
Bearing bar center:20
Open Aera:42%
Approx Weight:10.5kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP Molded Grating 20*20H14 is suitable for walkways, platforms, trench covers and equipment operating surfaces that require slip resistance, corrosion resistance and load bearing. It is commonly used in humid or chemically exposed environments such as chemical processing, water treatment, electroplating and marine engineering. Its 20*20 mm mesh and H14 thickness specification make it convenient to lay at conventional support spacing. Please contact us to confirm suitability for your specific operating conditions.
Selection Guidance
When selecting, please confirm the resin system (such as orthophthalic, isophthalic, vinyl ester or bisphenol A type) and the required flame retardant grade to match the corrosiveness of the medium and fire protection requirements. At the same time, check the grating thickness and mesh size against span, load and installation method. If you provide the operating environment and load conditions, we can assist in recommending a suitable configuration and provide specification details.
Product Advantages
Molded grating is formed in one piece from unsaturated polyester resin and fiberglass in a mold. The interwoven mesh structure distributes loads evenly, combining light weight, high strength and corrosion resistance, with a slip-resistant surface that is easy to cut and install. Compared with conventional metal grating, it resists rust better in humid and chemical environments and requires less maintenance.
Inquiry Guidance
For detailed specifications, resin selection and commercial terms for FRP Molded Grating 20*20H14, please contact us to obtain detailed specifications and a quotation. Please provide your operating environment, size requirements and quantity, and we will provide a corresponding solution and supply information.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English