Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*152*38(mm)
Panel size available:
1220*3660,1220*2440,915*3050 Length stress
Bearing bar thickness (Top/Bottom):9.0/6.5
Bearing bar center:25
Open Aera:63%
Approx Weight:22.5kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating 25*152 H38 is suitable for walkways, platforms, trench covers and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity, and is commonly used in chemical, water treatment, power and marine engineering environments. To confirm whether it fits your specific scenario, please contact our technical team for discussion.
Selection Guide
When selecting, it is necessary to consider whether the resin system (such as orthophthalic, isophthalic, vinyl ester or bisphenol A type), grating thickness and mesh size match the load and media conditions, and you may also confirm whether flame retardancy, a slip-resistant surface or special colors are required. As specific working conditions and parameters are involved, we recommend you provide your usage environment information so that we can assist with specification selection.
Product Advantages
This molded grating uses unsaturated polyester resin as the matrix with glass fiber reinforcement, offering light weight and high strength, chemical corrosion resistance, insulation and non-magnetic properties, and easy cutting and installation, with an optional slip-resistant surface treatment. Compared with traditional metal grating, it supports longer-term use and maintenance in humid or corrosive environments, with specific performance depending on the resin and formulation.
Inquiry Guide
For detailed specifications, suitable solutions and commercial terms for FRP molded grating 25*152 H38, please contact us for detailed specifications and a quotation. Please let us know your application environment, required dimensions and quantity, and we will provide selection recommendations and product information as soon as possible.
Operating Environment
- FRP molded grating with a 25×152 mm mesh and 38 mm depth is used in outdoor walkways, platforms and stair treads where UV exposure and weathering are continual, so the isophthalic or bisphenol-A resin options are chosen for their resistance to sunlight degradation.
- In industrial plants, this grating is installed over chemical process areas, drainage channels and wash-down zones, where the unsaturated polyester resin system and ATH filler resist splashes of acids, alkalis and solvents that would corrode steel.
- Because the fiberglass reinforcement does not rust, the grating is suitable for humid, condensation-prone and coastal atmospheres, including indoor pits and outdoor structures with frequent wetting.
- For high-temperature service or fire-sensitive locations, the phenolic resin grade listed in the resin table offers low toxicity and high flame retardant properties, suited to enclosed environments where smoke emission is a concern.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.