Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




26*26*38(mm)
Panel size available:
1150*4011 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.0/5.0
Bearing bar center:25
Open Aera:60%
Approx Weight:19.5kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP Molded Grating 26*26H38 is suitable for platforms, walkways, trench covers, stair treads and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity. It is commonly used in chemical, water treatment, power, marine engineering and general industrial workshop applications. For suitability under specific working conditions, please contact us to confirm based on media, loads and installation methods.
Selection Guide
When selecting, we recommend first clarifying the corrosive media and flame retardancy requirements of the service environment, then confirming the load-bearing requirements and support span, so as to make a suitable match among resin systems such as orthophthalic, isophthalic, vinyl ester or bisphenol A types, and different mesh and thickness specifications. You are welcome to contact us with your working conditions, and we will assist in recommending suitable grating models and structural solutions.
Product Advantages
The molded process forms the grating in one piece, with uniform distribution of fibers and resin. It combines lightweight, high strength, corrosion resistance, slip resistance, insulation and ease of cutting and installation, with low daily maintenance costs. Compared with traditional metal grating, it is less prone to rusting in humid, acid and alkaline environments and has a longer service life.
Inquiry Guide
If you would like to know the detailed specifications, resin system options, colors and surface treatments of FRP Molded Grating 26*26H38, please contact us for detailed specifications and quotations. Please provide information such as the service environment, load-bearing requirements and required quantity, and we will provide targeted selection advice and commercial solutions as soon as possible.
Operating Environment
- Because the molded FRP grating uses unsaturated polyester resin with glass fiber reinforcement, the 26×26H38 grating tolerates both indoor and outdoor exposure without the corrosion problems of metal gratings.
- It is suitable for humid, wet and chemically corrosive atmospheres, including areas where acids, alkalis or salts are present, depending on the resin selected (such as isophthalic, bisphenol or phenolic types).
- For installations exposed to continuous moisture, chemical splash or washdown, the phenolic-type resin option offers high flame retardancy with a high oxygen index, while standard grades handle general industrial weather and humidity.
- Contact us with your specific temperature, chemical and load conditions so we can recommend the appropriate resin grade for your floor, platform or walkway application.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

简体中文
English