FRP Molded Grating 38*152 H38
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
Fiberglass reinforced plastic (FRP) molded grating is a panel with a certain open area, made in a custom mold with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 33% | E |
Filler | 31% | ATH,PR |
Other | 1% | --- |
Resin type
Code | Resin type | Flame retardancy | Recommended applications |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index up to approximately 80 | Low toxicity and high flame retardancy; fire safety is very important in these applications |
VEFR-25 | Vinylester type | Oxygen index 28 and above | Harsh corrosive environments such as acids and alkalis |
VEFR-10 | Vinylester type | Oxygen index 35 and above | Applications with high acid and alkali exposure and high flame-retardant requirements |
IFR-25 | Isophthalic type | Oxygen index 28 and above | A VEFR economical grade, with good performance and resistance to moderate acids, alkalis and solvents |
IFGR-30 | Benzene-based, food grade | Oxygen index 26 | Mainly used for meat products and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index 28 and above | General acid and alkali environments |
OCR | Orthophthalic type | Oxygen index below 28 | OFR-25 economical grade, no flame retardancy requirement |
Chopped glass fiber selection
Code | Chopped strand mat type | Recommended applications |
E | E-glass | For high-strength requirements and high corrosion resistance applications |
Filler type selection
Code | Filler type | Recommended applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame retardant, smoke suppression and corrosion resistance applications |
PR | No filler, pure resin | For high corrosion resistance applications |




38*152*38(mm)
Available panel sizes:
1220*3660, 1220*2440, 915*3050 lengthStress
Load-bearing flat bar thickness (top/bottom): 8.0/6.0
Load-bearing flat bar center spacing: 38
Open area: 67%
Approximate weight: 15.92 kgs/m²

Line load (unit: mm)
Deflection | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Ultimate |
|---|---|---|---|---|---|---|---|
Span (mm) | 75 | 150 | 300 | 450 | 600 | 750 | Load |
| 300 | <0.25 | <0.25 | 0.25 | 0.51 | 0.51 | 0.76 | 12628 |
| 450 | <0.25 | 0.25 | 0.76 | 1.02 | 1.52 | 1.78 | 9946 |
| 600 | 0.25 | 0.76 | 1.52 | 2.29 | 3.05 | 3.81 | 8233 |
| 750 | 0.76 | 1.27 | 2.79 | 4.06 | 5.33 | 6.6 | 7040 |
| 900 | 1.02 | 2.29 | 4.32 | 6.64 | 8.64 | 10.9 | 6146 |
| 1050 | 1.52 | 3.3 | 6.6 | 9.91 | --- | --- | 5439 |
| 1200 | 2.29 | 4.83 | 9.65 | --- | --- | --- | 5141 |

Uniformly distributed load (unit: mm)
Deflection | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Ultimate |
|---|---|---|---|---|---|---|---|
Span (mm) | 350 | 450 | 750 | 1000 | 1500 | 2500 | Load |
| 300 | <0.25 | <0.25 | <0.25 | 0.25 | 0.25 | 0.51 | 41358 |
| 450 | <0.25 | 0.25 | 0.51 | 0.76 | 1.02 | 1.78 | 26962 |
| 600 | 0.51 | 1.02 | 1.27 | 1.78 | 2.79 | 4.57 | 21716 |
| 750 | 1.03 | 2.03 | 3.05 | 4.06 | 6.35 | --- | 18446 |
| 900 | 2.54 | 4.06 | 6.1 | 8.13 | 12.2 | --- | 13420 |
| 1050 | 4.57 | 7.11 | 10.7 | --- | --- | --- | 10180 |
| 1200 | 7.87 | 11.9 | --- | --- | --- | --- | 8418 |

Features:
Corrosion resistance
Slip resistance
Superior ergonomics
Low installation cost
Flame retardant
Lightweight, bidirectional strength, and easy cutting make the pipe easier to install.
Uniform color inside and out; colors can be selected freely.
Delivers favorable social and economic benefits.
Designable, flexible and varied in size, with stable dimensions
Widely used in:
Greenlogy TECFRP grating is widely used for industrial platform floors, stairs, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.
Application Scenarios
FRP molded grating 38*152H38 is suitable for operating platforms, walkways, trench covers and stair treads in petrochemical, power, wastewater treatment and marine engineering fields. Its corrosion resistance, light weight and high strength deliver excellent performance in humid, acid and alkali corrosive environments.
Selection Guide
Selection should consider load requirements, service environment (corrosive media, temperature) and safety needs (such as flame retardancy and anti-slip). Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) provide different corrosion resistance and flame retardancy, and can be selected according to specific working conditions. Contact us for detailed specifications and selection advice.
Product Advantages
FRP molded grating offers advantages such as light weight and high strength, corrosion resistance, anti-slip performance, insulation and maintenance-free operation, and colors and sizes can be customized on request. Its unique mesh structure makes installation and cutting easy, suitable for various complex applications.
Inquiry Guide
For more product information, technical parameters or a quotation, please contact us at any time. We provide professional technical support and customization services, and welcome your inquiry.
Service Environment
- Molded FRP grating 38*152H38 is suitable for outdoor and indoor service environments in industrial plants, and can replace steel grating where humidity and chemical corrosion shorten service life.
- The isophthalic, vinyl ester and bisphenol A polyester resin systems specified above are suitable for continuous contact with acidic, alkaline and saline media in chemical, wastewater treatment and coastal facilities.
- The E-glass fiberglass reinforcement and ATH / PR filler contents listed in the material table give molded grating dimensional stability under humid and wet conditions, along with rot resistance and corrosion resistance.
- The phenolic resin grade (MP-5) in the raw material list is suitable for areas with low toxicity and high flame retardancy requirements, such as tunnels, offshore platforms and confined spaces where fire safety requirements are relatively high.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.