Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*100*50(mm)
Panel size available:
1220*3660 Length stress
Bearing bar thickness (Top/Bottom):8.0/5.0
Bearing bar center:38
Open Aera:62%
Approx Weight:15.3kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating 38×100 H50 pultruded-look is suitable for platforms, walkways, trench covers and equipment operating surfaces that require slip resistance, corrosion resistance and load-bearing capacity, and is commonly used in chemical, water treatment, power and general industrial environments. Its 38×100 mm mesh and 50 mm thickness provide a flat surface with a pultruded-like appearance, making it easy to use in wet locations, areas prone to liquid accumulation, or places requiring frequent washing. If you have specific working conditions, please contact us to confirm a suitable solution.
Selection Guide
When selecting, it is recommended to first clarify the resin system (such as orthophthalic, isophthalic, vinyl ester or bisphenol A type) and flame retardant requirements, then determine the grating thickness and mesh specification based on load-bearing span, support method and installation fixing form. The 38×100 H50 pultruded-look balances load-bearing capacity and open area, making it suitable for projects that require a pultruded-like surface effect while maintaining the integrity of molded grating. Welcome to contact us for detailed specifications and selection advice.
Product Advantages
This grating uses unsaturated polyester resin as the matrix and glass fiber as reinforcement, and is lightweight, high-strength, corrosion-resistant, slip-resistant and insulating, while the pultruded-like surface treatment makes its appearance closer to pultruded profiles. The integrated molded structure reduces splicing and maintenance needs, making it suitable for occasions with long-term exposure to corrosive media or outdoor environments. Specific performance can be further evaluated based on your usage conditions.
Inquiry Guidance
For detailed specifications, resin selection, colors, packaging and transportation information of FRP molded grating 38×100 H50 pultruded-look, welcome to contact us for specifications and quotations. Please provide the usage environment, load-bearing requirements and quantity, and we will assist you in matching a suitable product solution.
Operating Environment
- This molded FRP grating (38*100H50, pultrusion-look surface) is built on an unsaturated polyester resin skeleton with E-glass fiber reinforcement, so it is intended for indoor and outdoor service where moisture and humid air are continuously present.
- The isophthalic, vinyl ester and bisphenol resin options make the grating suitable for installations exposed to corrosive media such as acids, alkalis and salt-laden atmospheres in chemical, plating and water-treatment plants.
- The phenolic-type resin option is designed for low-toxicity, high flame-retardant service conditions, including areas where fire safety is a primary concern.
- Typical working positions include walkways, platforms, stair treads and trench covers, both under direct sunlight and in covered process areas; contact us for the full parameter list for your specific site conditions.