Pultruded Grating T-1810

Pultruded Grating T-1810

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Nantong Greenlogy TEC Electronic Technology Co., Ltd.

  FRP pultruded grating is made with pultruded "I"- and "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, assembled through a defined process, with gaps left in the panel surface.  

Name

Content

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass fiber

65%

E

Filler

8%

ATH,PR

Other

2%

---

Raw material introduction 
Resin type

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy, for applications with high fire safety requirements

VEFR-25

Vinyl type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl type

Oxygen index 35 and above

Acid and alkali environments with high flame retardancy requirements and favorable service conditions

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical grade, with good performance and resistance to moderate acids, alkalis and solvents

IFGR-30

Food-contact grade, benzene type (styrene-based)

Oxygen index 26

Mainly used in meat product and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical grade, no flame retardant requirement

Coarse glass fiber selection   

Code

Coarse grit (sand) type

Recommended applications

E

Alkali-free (E-glass) sand

For applications requiring high strength and high corrosion resistance

Selected filler type  

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Applications requiring flame retardancy, smoke suppression and corrosion resistance

PR

No filler, pure resin

For high corrosion resistance applications

Software - Three-column example 1

Grit surface
Software - Three-column example 2

Smooth surface
Software - Three-column example 3

Anti-slip grooved surface

T1810

Standard panel size:
1220mm, 915mm wide; 3050mm, 6100mm long
Load-bearing flat bar: 25mm
Open area: 18%

Approx. weight (including three cross rods): 13.8kg/m²
Diagram of concentrated line load on FRP grating T-1810

Patch load (unit: mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

(mm)

300500800150020002500

Load

4000.40.671.0722.673.345900
6001.242.063.38.25------2300
8002.764.597.3513.8------2300
10005.168.613.8---------2200
Diagram of uniformly distributed load on FRP grating T-1810

Uniform load (unit: mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Ultimate

(mm)

300500800150020002500

Load

4000.10.170.270.50.670.8329600
6000.460.771.242.323.13.8712700
8001.382.33.676.899.1811.57300
10003.225.378.6---------4600

Features:

  • Flame retardant

  • High flame retardancy

  • Low smoke and low-toxicity smoke emission

  • High strength-to-weight ratio

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Electrical and thermal insulation

  • Easy to process

  • Impact resistant 

  • UV resistant

  • Maintenance-free

Installation and accessories

Installation and accessories

Application scenarios

Pultruded grating T-1810 is suitable for industrial platforms, walkways, stair treads, trench covers, and applications in wastewater treatment, chemical processing, marine engineering, and similar fields where load-bearing and corrosion resistance are required. Its structure is assembled from pultruded "I"- or "T"-shaped load-bearing bars with solid tubes or rods as connecting rods, offering light weight, high strength, corrosion resistance, and slip resistance. Please consult us regarding specific applicable environments based on your operating conditions.

Selection guide

When selecting, consider the resin type (such as orthophthalic, isophthalic, vinyl ester, or phenolic) to meet different corrosion resistance and flame-retardant requirements, and determine the grating thickness, opening (grid) size, load rating, and surface anti-slip treatment. Different resin systems correspond to different chemical resistance and flame-retardant performance; for example, phenolic resin offers low toxicity and high flame retardancy. Please contact us for detailed specifications and selection recommendations.

Product advantages

Pultruded grating T-1810 is formed by the pultrusion process, with high fiber content, offering excellent unidirectional strength and high stiffness. Compared with molded grating, pultruded grating provides higher strength in the load-bearing direction and is suitable for long-span applications. The product is corrosion resistant, maintenance-free, insulating, non-magnetic, and easy to install. Please consult us for specific performance parameters.

Inquiry guidance

For detailed specifications, technical parameters, pricing, and delivery times of pultruded grating T-1810, please contact us. Please provide your specific application requirements, and we will provide professional technical support and a quotation.

Operating environment

  • Pultruded FRP grating T-1810 is suitable for indoor and outdoor use in industrial plants, wastewater treatment facilities, chemical processing areas, and offshore platforms.
  • The pultruded FRP load-bearing bars and connecting rods resist moisture, humidity, and attack by a variety of highly corrosive chemical media, making the grating suitable for exposed and washdown environments.
  • When a flame-retardant resin system (such as phenolic or vinyl ester resin) is used, the grating can be used in areas with fire safety and low toxicity requirements.
  • For detailed recommendations on resin selection and environmental limits for your specific site conditions, please contact us.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.